Abstrakt: Conclusions 1.A study was made of the physicomechanical and antifriction properties of Fe-WSe2 composite materials produced by hot pressing.2.It was established that by subjecting precompacted specimens to hot pressing at 700°C it is possible to obtain material with a residual porosity of 1–3% (at WSe2 contents ranging from 5 to 30 wt.%) and high mechanical properties.3.The best antifriction properties in operation in air under dry friction conditions at sliding speeds of 0.05–3.0 m/sec are exhibited by composite materials containing 10–20% WSe2.