Autor: |
Petrov-Denisov, V. G., Pichkov, A. M., Shakhov, I. I., Matveev, Yu. V., Pozdnyakova, N. K. |
Zdroj: |
Refractories; March 1985, Vol. 26 Issue: 3-4 p170-173, 4p |
Abstrakt: |
Conclusions An accelerated drying and first heat up cycle was developed for a kiln unit for dry production of clinker with a capacity of 3000 tons/day with cyclone heat exchangers with a lining of refractory concretes of high-alumina cement with a chamotte aggregate. The drying of the lining and the heating of the unit were done in 4 days. The results of the work indicate the desirability of use of refractory concretes for lining the cyclone heat exchangers of kiln units for dry production of clinker. |