Autor: |
Kashcheev, I. D., Matyushina, V. R., Yudin, I. A., Sivash, V. G., Kovylov, V. M., Bykov, A. N. |
Zdroj: |
Refractories; March 1980, Vol. 21 Issue: 3-4 p208-211, 4p |
Abstrakt: |
Conclusions The authors have investigated aluminosilicate fiber with organosilicon binder. They show that a rise in pressing pressure from 5 to 50 kPa, a rise in temperature from 300 to 500°C, and a rise in treatment time from 15 to 60 min enables us to obtain products with apparent densities from 0.4 to 0.65 g/cm3. |
Databáze: |
Supplemental Index |
Externí odkaz: |
|