Autor: |
Popov, A. D., Chukreeva, E. I., Flyagin, V. G., Mikhailov, Yu. F., Dyban', Yu. P., Salganik, M. D., Makarychev, A. R., Pesina, N. M. |
Zdroj: |
Refractories; May 1969, Vol. 10 Issue: 5-6 p265-268, 4p |
Abstrakt: |
Conclusions The Barzassk (basic O1 and O2, and semiacid PK1) clays are suitable for making chamotte and semiacid ladle brick. The production of refractories from these clays can be organized using the technological production scheme for chamotte articles made by semidry pressing. In order to increase the strength of the green products made from semiacid clays it is necessary to reprocess the bodies with an addition of sulfite lye on runner mixers with rollers. |