Autor: |
Cui, B. Z., Sui, Y. C., Sun, X. K., Xiong, L. Y., O’Shea, M. J., Zhang, Z. D. |
Předmět: |
|
Zdroj: |
Journal of Applied Physics; 5/15/2002 Part 1, 2 & 3, Vol. 91 Issue 10, p7881, 3p, 1 Black and White Photograph, 3 Charts, 3 Graphs |
Abstrakt: |
The relationship between the phase evolution, nanostructure, exchange coupling, and magnetic properties of Nd[sub 8.4]Fe[sub 86]Mo[sub l.1]B[sub 4.5] magnets prepared by melt spinning (MS) and mechanical milling (MM) are studied by x-ray diffraction, Mössbauer spectroscopy, positron lifetime measurements, high resolution transmission electron microscopy observations, and magnetization measurements. The maximum magnetic energy product (BH)[sub max] for MM magnets annealed at 650 °C or below are notably higher than those of the corresponding MS samples due to the larger amount of the Nd(Fe,Mo)[sub 7] present in the MS samples. [ABSTRACT FROM AUTHOR] |
Databáze: |
Complementary Index |
Externí odkaz: |
|