Long-term Evaluation of Bonding Performance of Universal Adhesives based on Different Dentinal Moisture Levels.

Autor: de Faria Nonato, Rammon, de Aguiar Moreira, Pedro Henrique, de Oliveira da Silva, Daniella, Cantanhe de Ferreira, Michel Wendlinger, Reis, Alessandra, Millan Cardenas, Andres Felipe, Loguercio, Alessandro D., Figuerêdo de Siqueira, Fabiana Suelen
Zdroj: Journal of Adhesive Dentistry; 2022, Vol. 24 Issue 1, p395-405, 11p
Abstrakt: Purpose: To evaluate the microtensile bond strength (µTBS) and silver nitrate uptake (SNU) of three universal adhesives used in etch-and-rinse (ER) and self-etch (SE) modes on dry, wet, and oversaturated dentin surfaces after 24 h and 1 year of water storage. The morphology of the hybrid layer (MHL) and the degree of conversion (DC) were also evaluated. Purpose: To evaluate the microtensile bond strength (µTBS) and silver nitrate uptake (SNU) of three universal adhesives used in etch-and-rinse (ER) and self-etch (SE) modes on dry, wet, and oversaturated dentin surfaces after 24 h and 1 year of water storage. The morphology of the hybrid layer (MHL) and the degree of conversion (DC) were also evaluated. Results: When 24-h vs 1-year data were compared, there was a significant decrease in µTBS and an increase in SNU values for the majority of experimental groups (p < 0.0001). On dry (ER) and oversaturated (ER and SE) dentin, AMB showed higher µTBS than did PBA (p < 0.00001). No significant decrease in µTBS was observed when universal adhesives were applied in the SE mode to dry dentin (p > 0.05). Regarding SNU, at all moisture levels, AMB showed lower SNU values than SBU (p < 0.001). Regarding MHL, SBU showed several imperfections when applied to oversaturated dentin in comparison with AMB and PBA. Regarding DC, when dentin was kept dry or was oversaturated, AMB showed a higher DC than PBA (p < 0.0001). Conclusion: The behavior of the different universal adhesives evaluated did not vary when applied to wet or dry dentin. However, the results with oversaturated dentin were dependent on the universal adhesive. Independent of the moisture level and the universal adhesive evaluated, significant degradation of the bonding properties occurred after 1 year of water storage, with the exception of universal adhesives applied to dry dentin in the SE strategy. [ABSTRACT FROM AUTHOR]
Databáze: Complementary Index