Evaluating the Solubility of Endodontic Sealers in Response to Static and Dynamic Stress: An In Vitro Study.

Autor: SAGHIRI, Mohammad Ali, AMANABI, Mahsa, SAMADI, Elham, ASATOURIAN, Armen, SAMADI, Fatereh, MORGANO, Steven M.
Předmět:
Zdroj: European Endodontic Journal; Aug2024, Vol. 9 Issue 3, p231-235, 5p
Abstrakt: Objective: This study investigated the effect of static and dynamic conditions on the solubility of three endodontic sealers: AH Plus (an epoxy-resin-based sealer), Bio-C Sealer (a bioceramic sealer), and EndoSequence BC (a bioceramic sealer). Methods: Plastic moulds were used to create 150 specimens, which were divided into three groups, with each group being filled with one of the three sealers. After the setting time, the specimens were removed from the moulds, dried, and weighed. Thirty specimens from each group were subdivided into three subgroups and stored in distilled water for 30, 60, or 90 days, while the remaining 20 specimens in each group were subdivided into four subgroups and subjected to 0, 20, 50, or 100 thermocycling cycles. After storage time and thermocycling, the specimens were reweighed, and the weight loss and solubility percentage were calculated. The data were analysed using one-way ANOVA, Post Hoc Tukey, and Pearson correlation tests (p<0.05). Results: The results showed that AH Plus had the lowest solubility, followed by EndoSequence BC and then Bio-C Sealer (p<0.0001). Both static and dynamic conditions had a negative effect on the solubility of all tested sealers, with the effect being more pronounced in bioceramic sealers. The increase in storage days and the number of thermocycling cycles were significantly correlated with the increasing solubility levels of all tested sealers (p<0.0001). Conclusion: The increased solubility of endodontic sealers may have a negative impact on long-term treatment outcomes. Both static and dynamic conditions can affect the solubility of endodontic sealers. [ABSTRACT FROM AUTHOR]
Databáze: Complementary Index