Autor: |
G, Veeraiah, N, Ramanaiah, I, Sudhakar, K, Venkateswarlu |
Předmět: |
|
Zdroj: |
Advances in Materials & Processing Technologies; Dec2022, Vol. 8 Issue 4, p4095-4105, 11p |
Abstrakt: |
Dissimilar weld made of AA5083 and AA 7075 aluminium alloys using TIG welding (Current inthe range of 80120 amps) has investigated. Ultimate tensile strength of different weld joints fabricated at different current considered for assessing the joint quality. The results demonstrated that an optimum weld current of 100 amp yielded ~ 283 MPa tensile strength. Compositional analysis across weld pool has shown a signature of Mg vaporisation and Zn retention resulting in yielding high weld strength. The dilution curves of the Zn in 7075 side of TIG welded specimens show a gradual decrease in Zn fraction in HAZ leads to failure of tested samples along the HAZ side of AA7075. It has found that in the weld microstructure,there is a tendency in the weld zone for stabilising Mg by forming various intermetallic phases. [ABSTRACT FROM AUTHOR] |
Databáze: |
Complementary Index |
Externí odkaz: |
|