Autor: |
Popov, A. G., Kolodkin, D. A., Gaviko, V. S., Vasilenko, D. Yu., Shitov, A. V. |
Předmět: |
|
Zdroj: |
Metal Science & Heat Treatment; Nov2018, Vol. 60 Issue 7/8, p528-533, 6p |
Abstrakt: |
Two groups of sintered permanent magnets with reduced temperature coefficient of induction (TCI) are considered, i.e., (A ) (Nd0.64Dy0.36)16(Fe1 - xCox)77.5Cu0.1Ga0.3B6.1(x = 0.22 - 0.36) and (B) Nd0.64 - zDy0.36Hoz)16(Fe0.64Co0.36)77.5Cu0.1Ga0.3B6.1 ( z = 0.08 - 0.26). It is shown that substitution of 36% Fe by Co raises the Curie temperature of the magnets to 576°C and lowers the TCI to ∣ − 0.02 ∣ % /K in the range of 27 - 120°C. Substitution of Nd by Ho lowers the TCI additionally to zero at z = 0.17 and changes it to ∣ + 0.009 ∣ % /K at z = 0.26. The results of the study of the phase composition and of the microstructure of the magnets make it possible to explain the observed lowering of the coercivity under the alloying. [ABSTRACT FROM AUTHOR] |
Databáze: |
Complementary Index |
Externí odkaz: |
|
Nepřihlášeným uživatelům se plný text nezobrazuje |
K zobrazení výsledku je třeba se přihlásit.
|