Glass ionomer cement (GIC) has limitation on the mechanical properties especially compressive strength. The change of compressive strength of GIC by adding oxalic acid and tartaric acid has been investigated. Oxalic acid and tartaric acid was added to the liquid components at concentrations of 0 - 15% (w/w). Powder component of GIC was made from optimum experimental powder glass SiO2-Al2O3-CaF2. GIC was characterized by compressive strength test, SEM-EDX and FTIR. The addition of tartaric acid to GIC has greater improvement than addition of oxalic acid. The addition of tartaric acid at 10 % (w/w) to GIC has greatest value of compressive strength. [ABSTRACT FROM AUTHOR] |