Pulpal Temperature Variances During Step-by-step Adhesive Restorative Procedure Using Three Different High-irradiance Light-curing Units.
Autor: | Nakagawa RK; Rodrigo Keigo Nakagawa, DDS, MSc, PhD, postdoctoral researcher, Department of Restorative Dentistry, Federal University of Minas Gerais, Bel o Horizonte, Brazil., Araújo de Oliveira HH; Hans Hatner Araújo de Oliveira, DDS, MSc student, Department of Restorative Dentistry, Federal University of Minas Gerais, Belo Horizonte, Brazil., Abreu LG; Lucas Guimarães Abreu, DDs, MSc, PhD, professor, Department of Pediatric Dentistry, Universidade Federal de Minas Gerais., R CA; Rodrigo de Castro Albuquerque, DDS, MSc, PhD, professor, Department of Restorative Dentistry, Federal University of Minas Gerais, Belo Horizonte, Brazil., Lf DSAM; Luís Fernando dos Santos Alves Morgan, DDS, MSc, PhD, professor, Department of Restorative Dentistry, Federal University of Minas Gerais., A NM; Allyson Nogueira Moreira, DDS, MSc, PhD professor, Department of Restorative Dentistry, Federal University of Minas Gerais, Belo Horizonte, Brazil. |
---|---|
Jazyk: | angličtina |
Zdroj: | Operative dentistry [Oper Dent] 2024 Jan 01; Vol. 49 (1), pp. 43-51. |
DOI: | 10.2341/22-045-L |
Abstrakt: | The rise in temperature in pulp tissues is related not only to heat transfer by high-irradiance light-curing units (LCUs), but also to restorative procedures. This research aimed to compare the rise in pulp temperature (PT) induced by three LCUs at each restorative step while considering the influence of resin composite shade and thickness. To accomplish this, the investigators used a proposed experimental model replicating pulp fluid circulation with a controlled, simulated intraoral temperature in bovine incisors. The recorded external and internal PT ranged from 36.7°C to 37.1°C and 32.7°C to 33.0°C, respectively. A significant decrease of internal temperature was recorded during class V preparation, followed by a progressive and representative rise of temperature in the subsequent restorative steps. The temperature was significantly higher during light curing of the adhesive system using Valo compared to light curing using Elipar and Radii Cal. However, none of the analyzed devices produced a temperature that exceeded the pulp tolerance limit (a temperature increase over 5.5°C). The paired test showed no significant difference in pulp temperature associated with the thickness of the increment of resin composite. However, shade was found to have more influence on the amount of energy absorbed by pulp tissue-A1 samples showed significantly higher temperature variation compared to samples using the A4 shade of resin composite. To conclude, the microcirculation and the performance of procedures under constant air-water flux dissipate the heat absorbed by the pulp. Additionally, the data suggest that all three LCUs analyzed can be safely used in clinical procedures, and that the resin composite shade may influence the amount of irradiance delivered to the tooth surface and represents a significant factor in pulp temperature variance. (©Operative Dentistry, 2024.) |
Databáze: | MEDLINE |
Externí odkaz: |