Polyurethane Recycling: Thermal Decomposition of 1,3-Diphenyl Urea to Isocyanates.

Autor: Zamani S; Sustainable Process Technology, Faculty of Science and Technology, University of Twente, Drienerlolaan 5, 7522 NB Enschede, The Netherlands., van der Voort SHE; Sustainable Process Technology, Faculty of Science and Technology, University of Twente, Drienerlolaan 5, 7522 NB Enschede, The Netherlands., Lange JP; Sustainable Process Technology, Faculty of Science and Technology, University of Twente, Drienerlolaan 5, 7522 NB Enschede, The Netherlands.; Shell Global Solutions International B.V., Shell Technology Centre Amsterdam, Grasweg 31, 1031 HW Amsterdam, The Netherlands., Kersten SRA; Sustainable Process Technology, Faculty of Science and Technology, University of Twente, Drienerlolaan 5, 7522 NB Enschede, The Netherlands., Ruiz MP; Sustainable Process Technology, Faculty of Science and Technology, University of Twente, Drienerlolaan 5, 7522 NB Enschede, The Netherlands.
Jazyk: angličtina
Zdroj: Polymers [Polymers (Basel)] 2023 May 30; Vol. 15 (11). Date of Electronic Publication: 2023 May 30.
DOI: 10.3390/polym15112522
Abstrakt: Substituted urea linkages are formed during the production of polyurethane foam. To chemically recycle polyurethane toward its key monomers via depolymerization (i.e., isocyanate), it is essential to break the urea linkages to form the corresponding monomers, namely, an isocyanate and an amine. This work reports the thermal cracking of a model urea compound (1,3-diphenyl urea, DPU) into phenyl isocyanate and aniline in a flow reactor at different temperatures. Experiments were performed at 350-450 °C, with a continuous feed of a solution of 1 wt.% DPU in GVL. In the temperature range studied, high conversion levels of DPU are achieved (70-90 mol%), with high selectivity towards the desired products (close to 100 mol%) and high average mole balance (∼95 mol%) in all cases.
Databáze: MEDLINE
Nepřihlášeným uživatelům se plný text nezobrazuje