Autor: |
Alrefaie T; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan., Abdou A; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan.; Prosthodontic Dentistry Department, Division of Biomaterials, Faculty of Dentistry, King Salman International University, El Tur 46512, Egypt., Almasabi W; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan., Qi F; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan., Nakamoto A; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan., Nakajima M; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan., Otsuki M; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan., Shimada Y; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45, Yushima, Bunkyo-ku, Tokyo 113-8549, Japan. |
Abstrakt: |
This study investigated the effect of water sorption and bleaching on light transmission properties (Straight-light transmission (G0), Light diffusion (DF) and Amount of transmitted light (AV)) and translucency parameters (TP) of nano-filled flowable composites. A total of 35 composite disks (0.5 mm thickness) were prepared using A2 shade of 5 nanofiller composites (n = 7/each); Beautifil Flow Plus X F03 (SHOFU INC), Clearfil Majesty ES Flow (Kuraray Noritake Dental), Estelite Universal Flow (EUF, Tokuyama Dental), Estelite Flow Quick (Tokuyama Dental) and Filtek Supreme Ultra Flowable Restorative (FSU, 3M ESPE). Then, they were cured by LEDs (VALO, Ultradent) on standard mood (1000 mW/cm2) for 20 s. Samples were tested for straight-line transmission (G0), diffusion (DF), the amount of transmitted light (AV) and (TP) immediately after 24 h (dry storage), after 1-week water storage and after each of the three cycles of in-office bleaching (HiLite, SHOFU INC). Result: G0, DF, AV and TP were significantly affected by different materials (p < 0.001). The AV of FSU increased significantly after the 1-week water storage, then after the second bleaching cycle (p < 0.001). The TP for EUF slightly decreased (p = 0.019) after 1-week water storage, then increased throughout bleaching. Conclusion: Ageing/bleaching conditions do not affect G0, DF, AV and TP. The compositional variation between nano-filler composites resulted in a significant difference between materials. |