Deformation Features of the Propagation of Cleavage Cracks in a Ferritic-Pearlite Microstructure in the Ductile to Brittle Transition Interval.

Autor: Kantor, M. M.1 (AUTHOR) mkantor@imet.ac.ru, Sudin, V. V.1 (AUTHOR), Solncev, K. A.1 (AUTHOR)
Zdroj: Inorganic Materials. Jun2021, Vol. 57 Issue 6, p641-653. 13p.
Databáze: Academic Search Ultimate