Effects of the cooling mode on the integrity and the multi-pass micro-scratching wear resistance of Hardox 500 ground surfaces.
Autor: | Bensaid, Kamel1 (AUTHOR), Dhiflaoui, Hafedh1 (AUTHOR), Bouzaiene, Hassen1 (AUTHOR), Yahyaoui, Houda1 (AUTHOR), Fredj, Nabil Ben1 (AUTHOR) benfredjnabil@gmail.com |
---|---|
Zdroj: | International Journal of Advanced Manufacturing Technology. Apr2021, Vol. 113 Issue 9/10, p2865-2882. 18p. 6 Black and White Photographs, 6 Charts, 12 Graphs. |