Abstract Background Recently, various kinds of heat-treated nickel-titanium (NiTi) glide path instruments have been manufactured. This study aimed to investigate design, phase transformation behavior, mechanical properties of TruNatomy Glider (#17/02), V Taper 2H (#14/03), and HyFlex EDM (#15/03) and compare torque/force generated during simulated glide path preparation with them. Methods The designs and phase-transformation behaviors of the instruments were examined via scanning electron microscopy (n = 3) and differential scanning calorimetry (n = 2). Their bending (n = 15), torsional (n = 15), and cyclic fatigue resistances (n = 15) were tested. The ultimate strength and distortion angle were obtained from torsional resistance test. The number of cycles to failure (NCF) was calculated from cyclic fatigue resistance test. The preparation of the glide path was simulated using a double-curved artificial canal (n = 15), and the maximum torque and screw-in forces were measured. Data except NCF was compared between brands with one-way ANOVA with Tukey’s honestly significant difference test. NCF was analyzed via Kruskal–Wallis and Mann–Whitney U tests. Results TruNatomy Glider had the greatest number of threads. TruNatomy Glider showed progressive taper, while V Taper 2H and HyFlex EDM had constant taper. The austenitic transformation-finish temperatures of all the instruments were above body temperature. V Taper 2H demonstrated significantly lower ultimate strength, higher distortion angle, and a higher number of cycles to failure compared with HyFlex EDM and TruNatomy Glider (p |
Databáze: |
Directory of Open Access Journals |
Externí odkaz: |
|