Performance of butyl rubber–based macroporous sorbents as passive samplers
Autor: | Sevil D. Yakan, Atilla Yılmaz, Oya S. Okay, Oguz Okay, Oktay E. Tureyen, Berkant Yetiskin |
---|---|
Rok vydání: | 2020 |
Předmět: |
Fluoranthene
chemistry.chemical_classification Cyclohexane Health Toxicology and Mutagenesis Polycyclic aromatic hydrocarbon General Medicine Butyl rubber 010501 environmental sciences Phenanthrene 01 natural sciences Pollution chemistry.chemical_compound chemistry Environmental Chemistry Pyrene Benzene 0105 earth and related environmental sciences Naphthalene Nuclear chemistry |
Zdroj: | Environmental Science and Pollution Research. 28:3766-3773 |
ISSN: | 1614-7499 0944-1344 |
DOI: | 10.1007/s11356-020-08945-4 |
Popis: | In this study, two macroporous butyl rubber (BR)-based sorbents prepared in benzene (H-BR) and in cyclohexane (L-BR) with different porosities were synthesized by cryogelation technique. Their performances as a passive sampler were studied and then compared with commercially available silicon rubber (polydimethylsiloxane, PDMS) passive sampler. For that aim, polycyclic aromatic hydrocarbon (PAH) absorption rates of the sorbents in the short-term and their accumulation capacities in the long-term periods were investigated. Four PAHs (naphthalene, phenanthrene, fluoranthene, and pyrene) with a different number of aromatic rings were utilized. The concentrations of the PAHs in solutions were quantified by fluorescence spectrophotometer. The results showed that the BR sampler prepared in benzene (H-BR) generally has the highest absorption rates for all PAHs. The rate constants k (h-1) of the H-BR, L-BR, and PDMS samplers were found as 1.07, 0.55, and 0.55 for naphthalene; 0.73, 0.16, and 0.09 for phenanthrene; 0.24, 0.26, and 0.08 for fluoranthene; and 0.97, 0.38, and 0.17 for pyrene, respectively. The highest PAH absorption capacity was found for the BR sorbents prepared in benzene for all PAHs. Thus, benzene was selected as the organic solvent rather than cyclohexane for further studies in the preparation of butyl rubber-based samplers. The H-BR possessing the highest absorption rate and capacity underlines their usage as a capable passive sampler for both short- and long-term monitoring activities in the aquatic environments. |
Databáze: | OpenAIRE |