Choice of a rational scheme for casting of a forging ingot for producing hollow forgings.

Autor: Kolodkin, M., Zhul'ev, S., Dub, V., Romashkin, A., Mal'ginov, A.
Zdroj: Russian Metallurgy (Metally); Jun2010, Vol. 2010 Issue 6, p544-547, 4p
Abstrakt: The solidification of large ingots is simulated, and the results are confirmed in experiments. The application of cold-tapped direct-taper ingots is found to increase the ingot-to-product yield by 7% for the production of hollow billets and to decrease the degree of segregation heterogeneity in an ingot. The total carbon segregation in a cold-tapped ingot is three times lower than that in a comparative ingot. [ABSTRACT FROM AUTHOR]