Effect of Hydrofluoric Acid Concentration on Bond Strength to Glass-Ceramics: A Systematic Review and Meta-Analysis of In-Vitro Studies.
Autor: | Araújo-Neto VG, Nobre CFA, Freitas MIM, Lima RBW, Sinhoreti MAC, Del Bel Cury AA, Giannini M |
---|---|
Jazyk: | angličtina |
Zdroj: | The journal of adhesive dentistry [J Adhes Dent] 2023 Nov 17; Vol. 25, pp. 231-240. Date of Electronic Publication: 2023 Nov 17. |
DOI: | 10.3290/j.jad.b4646943 |
Abstrakt: | Purpose: To conduct a systematic review and meta-analysis of in-vitro bond strength to glass-ceramics using hydrofluoric acid (HF) at lower (<5%) and higher (>5%) concentrations ([HF]) to treat ceramic surfaces. Methods: Systematic searches were carried out in PubMed, Scopus, LILACS, and Web of Science for articles published through July 2021, and a meta-analysis was performed to estimate the combined effect by comparing the differences between the standardized means of the bond strengths of the evaluated materials. Results: In total, 943 articles were found, of which 17 studies were selected for qualitative analysis and 12 for quantitative analysis. The bond strength to glass-ceramics using 4% to 5% HF did not differ from that using 7% to 10% HF for the following HF etching times and glass-ceramic materials: 20 s for lithium-disilicate (Z = 0.65, p = 0.51), 60 s for feldspathic (Z = 0.53, p = 0.60), and 60 s for leucite (Z = 0.72, p = 0.35). Conclusion: The lower concentration HF (<5%) etchant is a reliable surface treatment for adhesive bonding to glass-ceramics with satisfactory bond strength in short-term evaluations. |
Databáze: | MEDLINE |
Externí odkaz: |