Zobrazeno 1 - 10
of 4 201
pro vyhledávání: '"wire mesh"'
Publikováno v:
Scientific Reports, Vol 14, Iss 1, Pp 1-16 (2024)
Abstract Sandwich panels with trapezoidal metal/glass fiber cores are increasingly popular due to their lightweight and energy-absorption properties. This study employs response surface methodology (RSM) and Box-Behnken design to investigate the effe
Externí odkaz:
https://doaj.org/article/ce2a705354e249a8a70272f36c2f3df8
Publikováno v:
Iranian Journal of Electrical and Electronic Engineering, Vol 20, Iss 3, Pp 141-154 (2024)
This paper proposes a structure for concrete composite materials that effectively attenuates transmitted power through the composite slab across a wide frequency range. The proposed structure is practical for electromagnetic interference shielding ap
Externí odkaz:
https://doaj.org/article/0b3d244861c84acf8c5935b40240ac69
Publikováno v:
International Journal of Concrete Structures and Materials, Vol 18, Iss 1, Pp 1-20 (2024)
Abstract In this paper, the shear behavior of ferro-cement hollow beams is investigated experimentally and analytically. Ten reinforced concrete beams with cross-sectional dimensions of 100 × 200 × 1300 mm and a clear span of 1000 mm were cast and
Externí odkaz:
https://doaj.org/article/7c11207cc21b4078b725a744aa0855db
Publikováno v:
Meitan xuebao, Vol 49, Iss 7, Pp 3216-3224 (2024)
The O2/CO2 combustion technology is a clean coal-fired power generation technology. However, a large amount of alkali metals released during the combustion of high-alkali coal is usually an important substance that causes ash deposition, slagging and
Externí odkaz:
https://doaj.org/article/8c9cf28ba6814f91959f51274c4d97f1
Publikováno v:
Frattura ed Integrità Strutturale, Vol 18, Iss 69, Pp 71-88 (2024)
Partial confinement can provide sufficient reinforcement to enhance the compressive strength and ductility of concrete with lesser confining material. This paper presents the results of an axial compression test conducted on eighteen plain concrete c
Externí odkaz:
https://doaj.org/article/4a8309a6a6804b07822db2180888de8e
Autor:
Elayaraja R, Rajamurugan G
Publikováno v:
Results in Engineering, Vol 24, Iss , Pp 103141- (2024)
This review examined the current developments in wire mesh reinforced natural fiber composites (WMRCs), emphasizing their material properties, applications, and production techniques. WMRCs provide a sustainable and economical alternative to conventi
Externí odkaz:
https://doaj.org/article/1ede86a8c0f8469eb9d689d79b2929b3
Publikováno v:
Journal of Advanced Mechanical Design, Systems, and Manufacturing, Vol 18, Iss 5, Pp JAMDSM0072-JAMDSM0072 (2024)
One pulse one wire mode was proposed for butt welding ultrafine 304 stainless steel wire mesh by pulsed microplasma arc welding. The weld morphologies and the resultant microstructure and mechanical properties were investigated. The results show that
Externí odkaz:
https://doaj.org/article/5b2a06499120430aba4fe49bb4b6b118
Publikováno v:
Alexandria Engineering Journal, Vol 94, Iss , Pp 257-273 (2024)
The current work investigates the effects of drilling parameters on hole quality, including delamination and circularity, produced in hybrid composite materials consisting of neat glass fibre (NG) and hybrid glass fibre/Al-wire mesh in two distinct s
Externí odkaz:
https://doaj.org/article/c53936c0eab5419b83a84a753db07d8d
Autor:
Misgina Mebrahtom, Yewuhalashet Fissha, Mujahid Ali, Angesom Gebretsadik, Yemane Kide, Zaid Nguse, Zemicael Gebrehiwot, Erick Saavedra Flores, Siva Avudaiappan, Hajime Ikeda
Publikováno v:
Scientific Reports, Vol 14, Iss 1, Pp 1-17 (2024)
Abstract Recent and past studies mainly focus on reducing the dead weight of structure; therefore, they considered lightweight aggregate concrete (LWAC) which reduces the dead weight but also affects the strength parameters. Therefore, the current st
Externí odkaz:
https://doaj.org/article/e51f70eff9f24bd0a594cfcb923b1f10
Publikováno v:
e-Polymers, Vol 24, Iss 1, Pp 1181-6 (2024)
To investigate the impact behavior and residual strength of glass fiber-reinforced polymer (GFRP) laminates embedded with/without steel wire mesh, low-velocity-impact (LVI) and post-impact tensile tests are conducted carefully. According to the wire
Externí odkaz: