Publikováno v:
Fenmo yejin jishu, Vol 41, Iss 5, Pp 434-441 (2023)
A novel nickel-based powder metallurgy superalloy FGH4113A (WZ-A3) was used to manufacture the full-size turbine disks by the process route of “vacuum induction melting + argon atomization + hot isostatic pressing + hot extrusion + isothermal forgi
Externí odkaz:
https://doaj.org/article/71aa6537f461422ba61988427e07cb3a
Autor:
Qingshuang Ma, Xintong Li, Ruifeng Xin, Enyu Liu, Qiuzhi Gao, Linlin Sun, Xuming Zhang, Chengxian Zhang
Publikováno v:
Journal of Materials Research and Technology, Vol 26, Iss , Pp 4168-4178 (2023)
At present, the operating temperature of the fourth-generation of nickel-based powder superalloys has not reach the target of 815 °C, and the traditional superalloy design and optimization methods are costly and inefficient. To overcome these challe
Externí odkaz:
https://doaj.org/article/7725772c43c94dcbbed95667d4b11e8f
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.