Nuclear Engineering and Technology, Vol 56, Iss 9, Pp 3942-3949 (2024)
This study focuses on investigating the chemical degradation characteristics of cementitious barriers used in low- and intermediate-level radioactive waste repository by reactive transport modeling. The impact of the blending with supplementary cemen
Externí odkaz:
https://doaj.org/article/24f80c1d43b44c279aae22c8a1240465
Publikováno v:
Case Studies in Construction Materials, Vol 21, Iss , Pp e03399- (2024)
In the long-term service process of Glass Fiber Reinforced Polymer – Reinforced Concrete (GFRP-RC) structures, degradation of GFRP bars and concrete materials can occur, leading to a partial loss of the internal bonding performance of the structure
Externí odkaz:
https://doaj.org/article/5d9891b6dded40a79557680797a0a5aa
Publikováno v:
BioResources, Vol 19, Iss 2, Pp 3180-3190 (2024)
Several commercial wood-based composites (softwood plywood [SWP], hardwood plywood [HWP], medium-density fiberboard [MDF], oriented strand board [OSB], and particleboard) [PB]) were post-treated with alkaline copper quat and copper azole at two diffe
Externí odkaz:
https://doaj.org/article/529c095bfec6415db11a4ebba29aac00
Autor:
Shifeng Qin, Kaiqi Li, Mengxue Cao, Wuhua Liu, Zhongyuan Huang, Guanjie He, Ivan P. Parkin, Huanxin Li
Publikováno v:
Nano Research Energy, Vol 3, Iss 3, p e9120122 (2024)
The non-noble metal (Fe, Co, Ni, etc.) catalysts possess promising potential to replace noble metals (e.g., Pt, Ru, Ir, etc.) as catalysts for oxygen electrocatalysis. Up to now, various mono- and dual-single-atom catalysts have been fabricated, thou
Externí odkaz:
https://doaj.org/article/4f269bc9fbc1473a8537f8bbf44e17ba
Autor:
Van Pho Nguyen, Wai Tuck Chow, Sunil Bohra Dhyan, Bohan Zhang, Boon Siew Han, Hong Yee Alvin Wong
Publikováno v:
Robotics, Vol 13, Iss 9, p 128 (2024)
Our study presents a novel design for a cable-driven robotic arm, emphasizing low cost, low inertia movement, and long-term cable durability. The robotic arm shares similar specifications with the UR5 robotic arm, featuring a total of six degrees of
Externí odkaz:
https://doaj.org/article/2c986254acdb49ea81dfab4443a6332a
Autor:
François El Inaty, Bugra Aydin, Maryam Houhou, Mario Marchetti, Marc Quiertant, Othman Omikrine Metalssi
Publikováno v:
Applied Sciences, Vol 14, Iss 7, p 2831 (2024)
Placed in a sulfate-rich environment, concrete reacts with sulfate ions, influencing the long-term durability of reinforced concrete (RC) structures. This external sulfate attack (ESA) degrades the cement paste through complex and coupled physicochem
Externí odkaz:
https://doaj.org/article/c93465f5be2b44aeb4517dc55f38aa67
Autor:
Sungchul Yang
Publikováno v:
Applied Sciences, Vol 14, Iss 5, p 1845 (2024)
This Special Issue covers the latest research on fatigue, performance, and damage assessments of concrete. Concrete fatigue is known as a phenomenon characterized by the repetition of loads. The fatigue-based performance of concrete may be affected b
Externí odkaz:
https://doaj.org/article/cdf8375db92f4a5ca60227dd4f941f18
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.