Zobrazeno 1 - 10
of 20
pro vyhledávání: '"Zeqin Liang"'
Autor:
Pedro Bamberg, Gregor Gintrowski, Zeqin Liang, Alexander Schiebahn, Uwe Reisgen, Nico Precoma, Christoph Geffers
Publikováno v:
Journal of Materials Research and Technology, Vol 15, Iss , Pp 5569-5581 (2021)
7000 series aluminum alloys have particularly high strength, if compared to other aluminum alloys or even to some high strength steels. Currently, this alloy is considered on the next developments of automotive structures, as an enabler of improved m
Externí odkaz:
https://doaj.org/article/abcfd93d49e540b3b34dba10e3d42145
Publikováno v:
Data in Brief, Vol 27, Iss , Pp - (2019)
The effect of pre-ageing (PA) time and temperature on subsequent natural secondary ageing (NSA) and paint bake (PB) hardening of an AA6014 Al–Mg–Si alloy was systematically investigated, especially when both parameters change. A wide range of PA
Externí odkaz:
https://doaj.org/article/e64d0d4a937548cc84471fdae70588ec
Publikováno v:
In Materialia September 2019 7
Autor:
Nico Precoma, C. Geffers, Zeqin Liang, Pedro Bamberg, Gregor Gintrowski, Alexander Schiebahn, Uwe Reisgen
Publikováno v:
Journal of Materials Research and Technology, Vol 15, Iss, Pp 5569-5581 (2021)
7000 series aluminum alloys have particularly high strength, if compared to other aluminum alloys or even to some high strength steels. Currently, this alloy is considered on the next developments of automotive structures, as an enabler of improved m
Publikováno v:
Scripta Materialia. 190:179-182
During quenching of aluminium alloys from the solutionising temperature vacancies are partially conserved as excess vacancies, partially lost to vacancy sinks, the exact fractions depending on the cooling rate. Positron lifetime measurements in sampl
Preaging PA is an industrial routine that suppresses the deleterious effect of natural aging and enhances the final paint bake hardening of 6XXX aluminum alloys. In view of the different advantages of PA at high and low temperatures, the effects of p
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::d7be04b73bd6ff8a94f818decce3cd28
http://www.helmholtz-berlin.de/pubbin/oai_publication?VT=1&ID=109025
http://www.helmholtz-berlin.de/pubbin/oai_publication?VT=1&ID=109025
Publikováno v:
SSRN Electronic Journal.
The deleterious effect of natural ageing (NA) on subsequent artificial ageing (AA) of Al-Mg-Si alloys can be markedly reduced by adding small amounts of Sn owing to the strong interaction between Sn atoms and excess vacancies. The retarding effect of
Autor:
Eike Gericke, Konrad Fricke, Andreas Röhsler, Xingpu Zhang, David Leyvraz, Mazen Madanat, Zeqin Liang, Zi Yang, Yong Yan, Robert Wendt, Armin Hoell, Qianning Guo, Meng Liu, John Banhart, Chunhui Liu
Publikováno v:
MATEC Web of Conferences, Vol 326, p 01001 (2020)
Precipitation hardening involves solutionising, quenching and annealing steps, the latter often at various temperatures. The phenomena observed in Al-Mg-Si alloys are very complicated and partially not well understood. During and after quenching, sol
Publikováno v:
MATEC Web of Conferences, Vol 326, p 02005 (2020)
The influence of quench rate after solution heat treatment on the microstructure in the as-quenched state and subsequent ageing kinetics of alloy AA6014 was investigated by means of transmission electron microscopy, positron annihilation lifetime spe
Autor:
John Banhart, Mohamed Elsayed, Benedikt Körner, Xingpu Zhang, David Leyvraz, Zeqin Liang, Meng Liu
Publikováno v:
Materialia. 6:100261
The deleterious effect of natural ageing (NA) on subsequent artificial ageing (AA) of Al–Mg–Si alloys can be markedly reduced by adding small amounts of impurities such as Sn or In owing to their strong interactions with vacancies. The retarding