Zobrazeno 1 - 10
of 70
pro vyhledávání: '"Zdeněk Knésl"'
Publikováno v:
Communications, Vol 8, Iss 4, Pp 25-28 (2006)
The growth of the fatigue crack is dependent on the crack growth resistance of the material as a bulk property. The fatigue crack growth properties of a material are usually described by the correlation between a crack propagation rate, and a corresp
Externí odkaz:
https://doaj.org/article/5820fe4d37284ab09c2943ac592efa17
Publikováno v:
Key Engineering Materials. :445-448
In recent years, particle reinforced composites are widely used due their mechanical properties as construction materials, high-performance engineering materials or protective organic coatings. The paper was mainly focused on the estimating of the in
Publikováno v:
Key Engineering Materials. 586:146-149
The paper presents a methodology for the lifetime assessment of welded polymer pipes. A fracture mechanics analysis of a butt-welded joint is performed by simulating radial crack growth in the nonhomogenous region of the pipe weld. It was found that
Publikováno v:
Engineering Fracture Mechanics. 110:438-447
This paper deals with assessment of conditions of fracture initiation in singular stress concentrations that are modeled by a bi-material notch composed of two orthotropic materials. Within the assessment of the stress concentrators, the stability cr
Publikováno v:
Polymer Testing. 32:106-114
The failure mode termed long time brittle failure (due to slow crack growth – SCG) limits the lifetime of plastic pipes. There are now two main accelerated tests (PENT and FNCT) that enable us to estimate the lifetime of HDPE used in plastics pipes
Publikováno v:
Computational Materials Science. 64:244-247
The paper presents a fracture mechanics approach to estimation of a critical load of a bi-material structure. The structure is a simple composite disc where the inner cylinder is made of aluminum and the outer cylinder is made of filled epoxy resin.
Publikováno v:
Computational Materials Science. 64:225-228
Surface crack propagation in a thin soft protective layer on a massive stiffer substrate is analysed using generalised linear elastic fracture mechanics. The growth of the initial crack is considered in both forward and sideways directions and the in
Publikováno v:
Key Engineering Materials. :162-165
The multi-layered structure components of dissimilar materials are used in many engineering applications to protect the base structure from outer damage. Typical examples of coated structures are pipes with the dimensional addition of protective laye
Publikováno v:
Key Engineering Materials. :178-181
In many industrial applications it is necessary to predict fatigue lifetime of the structures where the stress field near the crack front have a three-dimensional nature. Due to the existence of vertex singularity in the point where the crack front t
Publikováno v:
Key Engineering Materials. :158-161
Secure and cost effective joining methods are key points for practical applications of plastic pipelines. The morphology and material structure of welded joints are complicated in comparison with the base pipe material. The formation of the weld is h