Publikováno v:
High Temperature Materials and Processes, Vol 33, Iss 6, Pp 495-498 (2014)
In this work, the microstructure evolution of the Nb-12Si-22Ti-14Cr-2Al-2Hf alloy (at.%) fabricated by liquidmetal-cooled directional solidification (LMC) was investigated and the solidification behaviors were discussed. The results revealed that the
Externí odkaz:
https://doaj.org/article/967bba7f32a04f33bb155a7d3e57364a
Publikováno v:
China Foundry, Vol 10, Iss 6, Pp 345-350 (2013)
An Nb-14Si-22Ti-4Cr-2Al-2Hf-0.15Y(at.%) alloy was prepared by directional solidification (DS) with liquid metal cooling, and the withdrawal rates selected were 1.2, 6, and 18 mm·min-1, respectively. The Influence of withdrawal rate and heat treatmen
Externí odkaz:
https://doaj.org/article/454e3e76d7254baf866cf0353df8993d
Publikováno v:
High Temperature Materials and Processes, Vol 32, Iss 2, Pp 113-118 (2013)
In this work, an Nb-14Si-24Ti alloy (at.%) was prepared by liquid-metal-cooled directional solidification (DS) and then heat treated (HT) at 1450°C for 100 h. The effects of the withdrawal rate and heat treatment on the microstructure were investiga
Externí odkaz:
https://doaj.org/article/b60f5e6571c347049e73e72a9936292f
Autor:
Zhang, Junyan, Webber, Matthew S., Pu, Yunqiao, Li, Zhenglong, Meng, Xianzhi, Stone, Michael L., Wei, Bingqing, Wang, Xueqi, Yuan, Sainan, Klein, Bruno, Seemala, Bhogeswararao, Wyman, Charles E., Ramasamy, Karthikeyan K., Thorson, Mike, Langholtz, Matthew H., Heyne, Joshua S., Koishybay, Aibolat, Adhikari, Shiba, Cao, Sufeng, Sutton, Andrew, Tuskan, Gerald A., Román-Leshkov, Yuriy, Ragauskas, Arthur J., Ling, Tao, Davison, Brian H.
Publikováno v:
In Green Energy & Environment September 2024
Publikováno v:
In Materials Science & Engineering A 29 April 2016 663:98-107
Publikováno v:
In Chinese Journal of Aeronautics April 2014 27(2):438-444
Publikováno v:
In Materials Science & Engineering A 10 January 2013 560:672-677
Publikováno v:
Intermetallics. 38:102-106
To obtain a homogenous and optimizing microstructure, non-equilibrium directionally solidified (DS) samples at high withdrawal rate were heat treated (HT). The heat treatments were carried out at 1500 °C for 3–100 h. The DS and HT samples consiste
Publikováno v:
In Materials Letters 1 February 2013 92:317-320
Publikováno v:
In Materials Letters 1 October 2012 84:124-127