Zobrazeno 1 - 8
of 8
pro vyhledávání: '"Yu. V. Mikhailik"'
Publikováno v:
Journal of Analytical Chemistry. 61:14-19
4-Hydroxybenzoic acid-imprinted polymers and corresponding reference polymers were synthesized with the use of 4-vinylpyridine, acrylamide, and methacrylic acid as functional monomers. The specific surface area of these materials was estimated, and t
Autor:
Yu. V. Mikhailik, Boris A. Trofimov, G. F. Myachina, Anastasiya G. Mal'kina, S. A. Korzhova, L. V. Sokolyanskaya, Terje A. Skotheim, Tamara I. Vakul'skaya
Publikováno v:
Russian Journal of Electrochemistry. 38:188-192
The electrochemical activity of new highly sulfurized polyconjugated polymers is studied. The polymers, polythienothiophene, poly(4,5,6,7-tetrathieno-4,5,6,7-tetrahydro-2,3-dehydrobenzothiophene), poly(6-methylthieno[2,3-b]pyridine-4-thione-5-thiol),
Autor:
Olga V. Petrova, T. I. Vakul\\'skaya, Yu. V. Mikhailik, A. M. Vasil\\'tsov, S. A. Korzhova, Boris A. Trofimov, Al'bina I. Mikhaleva, G. F. Myachina, Terje A. Skotheim
Publikováno v:
Russian Chemical Bulletin. 51:1709-1714
Polyacetylene obtained by the dehydrochlorination of polyvinyl chloride in the NaOH—DMSO system undergoes sulfurization with elemental sulfur at 120—300 °C to liberate hydrogen sulfide and to form electroconducting (0.7·10–12—5.8·10–15Sm
Autor:
Lyudmila V. Klyba, A. G. Mal\\'kina, G. F. Myachina, L. V. Sokolyanskaya, S. A. Korzhova, Valentina V. Nosyreva, Terje A. Skotheim, Boris A. Trofimov, T. I. Vakul\\'skaya, I. V. Rodionova, E. S. Stoyanov, Yu. V. Mikhailik
Publikováno v:
Russian Chemical Bulletin. 51:282-289
Poly(2-methyl-5-vinylpyridine) is sulfurized with elemental sulfur at 140—320 °C to release hydrogen sulfide and to give black lustrous powders (sulfur content up to 45%) possessing electric conductivity (6.4·10–11—1.6·10–7 S cm–1), para
Autor:
G. F. Myachina, A. G. Mal\\'kina, T. I. Vakul\\'skaya, L. V. Sokolyanskaya, Terje A. Skotheim, S. A. Korzhova, Yu. V. Mikhailik, I. P. Kovalev, Lyudmila V. Klyba, Boris A. Trofimov, E. S. Stoyanov
Publikováno v:
Russian Chemical Bulletin. 50:253-260
Polystyrene was exhaustively sulfurized with elemental sulfur at 190--370 °C to liberate hydrogen sulfide and to form black lustrous powders (the sulfur content was up to 67%) possessing conductivity (10–7--10–6 S cm–1 upon doping with I2), pa
Autor:
L. V. Sokolyanskaya, Anastasiya G. Mal'kina, Terje A. Skotheim, L. I. Boguslavskii, Yu. V. Mikhailik, S. A. Korzhova, I. P. Kovalev, Tamara I. Vakul'skaya, G. F. Myachina, Trofimov Boris A
Publikováno v:
Russian Chemical Bulletin. 49:870-873
Autor:
I. P. Kovalev, G. F. Myachina, Yu. V. Mikhailik, L. V. Andriyankova, Boris A. Trofimov, Anastasiya G. Mal'kina, Terje A. Skotheim, S. A. Korzhova, Tamara I. Vakul'skaya
Publikováno v:
Russian Chemical Bulletin. 48:459-462
Polydiethylsiloxane reacts with elemental sulfur at 300–320 °C (ZnCl2 slightly accelerates the process) with evolution of hydrogen sulfide and formation of black lustrous paramagnetic powders (sulfur content up to 38.50%), which possess a noticeab
Publikováno v:
Theoretical and Experimental Chemistry. 33:202-205
Mesophases were established for the first time in sodium and potassium 4-(trifluoromethyl)-3,6-dioxaperfluorooctanesulfonates (RofSO3−) and in their binary systems Na,K/RofSO3(I) and Na/NO3,RofSO3(II). An increase in the temperature range of the me