Zobrazeno 1 - 9
of 9
pro vyhledávání: '"Yu. N. Tsvetkov"'
Autor:
Yu. N. Tsvetkov, Ya. O. Fiaktistov
Publikováno v:
Industrial laboratory. Diagnostics of materials. 89:64-70
The possibility of using profilometry for determining the duration of the incubation period of polymeric materials upon their testing for cavitation wear is considered. Six polymeric materials were tested for cavitation wear: plexiglass, fluoroplasti
Publikováno v:
Russian Engineering Research. 42:10-17
Publikováno v:
Russian Engineering Research. 39:580-586
Test results are presented for the cavitational wear resistance of electrolytic chromium coatings and alloys used in the manufacture of cylinder blocks and bushing for diesel engines. A method is proposed for predicting the wear resistance by measuri
Publikováno v:
Metal Science and Heat Treatment. 39:156-163
In the process of use many parts are subjected to the impact action of abrasive particles contained in a flow (jet) of gas or liquid and ones present on the contacting surfaces in the form of an abrasive layer. Despite the large number of publication
Autor:
Yu. N. Tsvetkov, L. I. Pogodaev
Publikováno v:
Metal Science and Heat Treatment. 36:116-122
Aluminum-nickel bronzes are known to have a high cavitation-erosion resistance; this is especially true of bronzes containing 11–14% Al, which can be used to restore worn parts of hydraulic engines, marine engines, etc. Analysis of the few publicat
Publikováno v:
Chemical and Petroleum Engineering. 27:442-444
Autor:
Yu. N. Tsvetkov, V. V. Evdokimov
Publikováno v:
Metal Science and Heat Treatment. 33:3-5
1. After tempering at 600±10°C 6h steel 20KhN3MFA is satisfactorily machinable, and this tempering regime can therefore be recommended as preliminary heat treatment prior to machining. 2. A rapid method of determining the relative machinability of
Publikováno v:
Chemical and Petroleum Engineering. 28:424-425
Operating conditions of the components of drill bit supports are characterized by extremely high contact stresses reaching 6000MPa, rotational speed of up to I0 sec -I, and action of abrasive particles and surface-active substances. As a result, more
Publikováno v:
Chemical and Petroleum Engineering. 21:507-510
This paper investigates the mechanical properties, local plastic deformation, and character of failure of D5KhN2MFASh and 16KhN3MASh steels after different heat treatments. The chemical analyses of these steels are shown in a table. An analysis of th