Autor:
Zhu Xiao, Hai-gen Wei, Chuang-li Guo, Shen Gong, Yong-ru Wang, Jiang Yanbin, Qian-ru Yang, Meng Wang, Zhou Li
Publikováno v:
Transactions of Nonferrous Metals Society of China. 31:3039-3049
Cu–Fe alloys with different Fe contents were prepared by vacuum hot pressing. After hot rolling and aging treatment, the effects of Fe content on microstructure, mechanical properties and electrical conductivity of Cu–Fe alloys were studied. The
Autor:
Jiang Yanbin, Tianyang Luan, Zhu Xiao, Pang Yongjie, Shen Gong, Zhou Li, Guohui Chao, Yong-ru Wang, Zhaohan Jiang
Publikováno v:
Materials Science and Engineering: A. 826:142012
The effect of Si on the microstructure and properties of Cu–10Fe alloy was systematically studied in this paper. By adding 0.4 wt% Si to Cu–10Fe alloy, the mechanical properties, electric conductivity, thermal conductivity, saturation magnetizati
Publikováno v:
Applied Mechanics and Materials. 159:361-365
The effects of different solid-solution temperature (500, 600, 700, 800, 900°C) and holding time (0.5, 1, 1.5, 2h) on properties and microstructure of Cu-Zn-Al-Ni alloy were investigated experimentally. The result shows that the hardness of the allo
Publikováno v:
Advanced Materials Research. :1168-1174
The degassing and dedusting mechanism of La and Ce during non-vacuum melting process of Cu-Cr-Zr alloy were analyzed by thermodynamics. The gibbs free energy changes of reactions of La and Ce with some impurties such as O2, H2, S, P and Si, were calc
Publikováno v:
Advanced Materials Research. :868-874
The microstructure of Cu-37%Zn-2%Mn-1.6%Al-0.7%Fe-0.7%Si (mass fraction)alloy was studied by scan electron microscopy, X-ray and optical microscopy. The α phase ratio and micro-hardness of this alloy after aging treatment were investigated. The resu
Publikováno v:
Advanced Materials Research. :1456-1464
The hot deformation behavior of Cu-0.35Cr-0.15Zr (wt.%) alloy was investigated by hot compression tests using a Gleeble-1500D thermal simulator system. The tests were performed under the conditions of 700°С- 820°С temperature and 0.01-10s-1strain