Zobrazeno 1 - 9
of 9
pro vyhledávání: '"Yitong Shi"'
Publikováno v:
International Journal of Molecular Sciences, Vol 24, Iss 13, p 10640 (2023)
Pollen development and its fertility are obligatory conditions for the reproductive success of flowing plants. Sucrose transporter 3 (OsSUT3) is known to be preferentially expressed and may play critical role in developing pollen. A 31-bp InDel was i
Externí odkaz:
https://doaj.org/article/ee39d033de6f44b9a0a34c3a8ebe9cea
Autor:
Xiantian Liang, Wei Zhang, Yitong Shi, Wen Zhang, Hongyi Yang, Ping Huang, Lingyun Li, Qi Zhang, Wei Zheng, Xueyuan Chen
Publikováno v:
Journal of Materials Chemistry C; 4/21/2024, Vol. 12 Issue 15, p5538-5548, 11p
Autor:
YITONG SHI, ZIQI ZHU
Publikováno v:
Journal of Applied & Numerical Optimization; 2024, Vol. 6 Issue 1, p71-82, 12p
Publikováno v:
International Journal of Molecular Sciences; Volume 24; Issue 13; Pages: 10640
Pollen development and its fertility are obligatory conditions for the reproductive success of flowing plants. Sucrose transporter 3 (OsSUT3) is known to be preferentially expressed and may play critical role in developing pollen. A 31-bp InDel was i
Publikováno v:
2022 IEEE 2nd International Conference on Data Science and Computer Application (ICDSCA).
Autor:
Sudha Joseph, Cemal Cem Tasan, David Dye, Dylan Hall, Richard J. Chater, Jinwoo Kim, Haoxue Yan, Yitong Shi, Sarah Fearn
Polished surfaces of Ti-6Al-4V, the most commonly used titanium alloy, were observed to suffer from hydride growth and associated embrittlement during hydrogen charging, whereas rough surfaces suffered no such susceptibility. Direct microscopic analy
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::0918ae7dc048b470d031c1e1f637c474
http://hdl.handle.net/10044/1/99899
http://hdl.handle.net/10044/1/99899
Publikováno v:
Journal of Applied & Numerical Optimization; 2022, Vol. 4 Issue 3, p341-355, 15p
Autor:
Trevor C. Lindley, David Dye, Edward A. Saunders, Sudha Joseph, Yitong Shi, Adrian Walker, Rebecca Sandala
Publikováno v:
Corrosion Science. 187:109497
The mechanism of AgCl-induced stress corrosion cracking of Ti-6246 was examined at \SI{500}{\mega\pascal} and \SI{380}{\celsius} for \SI{24}{\hour} exposures. SEM and STEM-EDX examination of a FIB-sectioned blister and crack showed that metallic Ag w
Publikováno v:
MATEC Web of Conferences, Vol 321, p 04025 (2020)
Hot salt stress-corrosion cracking (HSSCC) of titanium alloys has been found in the presence of chloride and other halide salts. Here, a series of AgCl HSSCC tests on Ti-6246 were conducted using a two-point bending rig at 380-500°C to determine the