Autor:
Liang, Yan, Yao, Yong-Cheng, Zhao, Lei, Shi, Lin, Chen, Yang-Kun, Mok, Vincent CT, Ungvari, Gabor S., Chu, Winnie CW, Tang, Wai-Kwong
Publikováno v:
In Journal of Affective Disorders 1 January 2020 260:557-568
Autor:
Yong-Lai Shang, Xin-Yu Ren, Hai-Shui Ren, Shu-Jie Pang, Yong-Juan Jing, Yao-yong Cheng, Hua-Ping Xiong
Publikováno v:
Welding in the World. 66:1437-1446
Publikováno v:
Welding in the World. 65:713-719
Cf/SiC composites were joined to itself with (and without) Mo interlayer at 1150 °C for 10 min by Cu–Pd–V filler metal. For two kinds of the joints, after the interfacial reactions, continuous V–C layers and dispersive V–C particles were for
Publikováno v:
Welding in the World. 64:1933-1938
In this study, brazing experiments were carried out on 6063 aluminum alloy using Al-20Cu-5Si-2Ni filler alloy. Microstructure, mechanical property, and removing behavior of oxide film of the brazed joints were analyzed. The results revealed that the
Publikováno v:
Welding in the World. 64:1771-1778
For high-temperature joining of SiC ceramics, a multi-element AuPdCoMnNi alloy was designed and used as filler metal to join SiC ceramics to metal Mo. The brazing experiment was conducted under the condition of 1150 °C for 5 min and 10 min, respecti
Autor:
Bo Chen, Yong-Wang Kang, Chong Pei, Huaping Xiong, A. I. Ustinov, Xinyu Ren, Yao-Yong Cheng, Hai-Shui Ren
Publikováno v:
Acta Metallurgica Sinica (English Letters). 32:1142-1150
Diffusion bonding of refractory Nb–Si-based alloy was performed with Ni/Al and Ti/Al nanolayers under the condition of 1473 K/30 MPa/60 min. The NbSS/Nb5Si3 in situ composite with the nominal composition of Nb–22Ti–16Si–3Cr–3Al–2Hf was us
Publikováno v:
Welding in the World. 61:375-381
Dissimilar joining of Ti3Al-based alloy to Ni-based superalloy has been conducted with diffusion bonding method using Ni foil and TiNiNb alloy as interlayer. For the Ni foil, with the increase of bonding temperature, the joint strength increased firs
Publikováno v:
Welding in the World. 61:181-186
SiO2f/SiO2 composite was joined to Al2O3 ceramic using AgCu-Ti active filler at brazing temperature of 1153 K for 10 and 60 min, respectively, and sound joints were achieved. It was found that a thin reaction layer had been formed close to each of th
Publikováno v:
Welding in the World. 60:99-108
V-containing-active high-temperature brazing alloys were designed for ceramic joining, including PdCo–V, AuPdCoNi–V, AuCuPd–V, and CuPd–V system alloys. The joined ceramics or ceramic composites include Si3N4 ceramic, AlN ceramic, carbon fibe
Publikováno v:
Welding in the World. 59:911-915
An advanced technology for joining powder metallurgy (P/M) superalloy and single crystal (SC) superalloy is highly needed for fabricating a high-strength turbine bladed disk and the joints must meet the requirements of harsh working conditions. In th