Zobrazeno 1 - 6
of 6
pro vyhledávání: '"Xiao Xuan Pian"'
Autor:
Bing Bing Fan, Biao Zhao, Wen Li, Bing Sun, Chen Yang Wang, Bin Bin Wang, Rui Zhang, Xiao Xuan Pian, Hao Chen
Publikováno v:
Key Engineering Materials. :590-593
SiCp/Cu composites were prepared by vacuum hot-pressing at 770°C for 1.5 h under the pressure of 30MPa. The composites were enhanced by CNTs with different volume fractions from 0 vol. % to 4 vol. %. Three-step approach wrapping process was introduc
Publikováno v:
Key Engineering Materials. :88-92
A fast method of microwave pyrolysis was provided to prepare α-Al2O3 powders. Aluminum hydroxide and Aluminum ammonium sulfate doclecahydrate were used as raw materials to obtain α-aluminum oxide powder by microwave pyrolysis, respectively. Thermo-
Autor:
Ke Ke Guan, Wu Hao, Fang Lei Tong, Qian Nan Mao, Bing Bing Fan, Chen Yang Wang, Xiao Xuan Pian, Li Na Miao, Hao Chen
Publikováno v:
Key Engineering Materials. :97-100
CaO(15%)-ZrO2nano-powders were prepared by microwave pyrolysis in a multi-model chamber at the temperature ranging from 650°C to 800°C, with the precursor processed at different reaction temperature from 0°C to 80°C by chemical co-precipitation m
Publikováno v:
Key Engineering Materials. :323-326
The industrial watchcases of 5Y-Tetragonal ZrO2were prepared by microwave sintering. Samples were sintered in a microwave chamber with TE666 resonant mode at 2.45GHz. The sintering temperature was from 1250°C to 1400°C. XRD and SEM techniques were
Autor:
Xiao Xuan Pian, Hao Chen, Bing Sun, Bing Bing Wang, Biao Zhao, Bing Bing Fan, Liang Zhang, Chen Yang Wang, Rui Zhang, Wen Li
Publikováno v:
Key Engineering Materials. :230-233
In this project, coal fly ash was transformed into ceramic materials by adding a certain amount of fusing agent. Ash samples were compacted and sintered with the addition of potassium carbonate (K2CO3·1/2H2O) under a suitable sintering temperature r
Autor:
Chen Yang Wang, Bing Sun, Xiao Xuan Pian, Hao Chen, Bing Bing Fan, Biao Zhao, Xin Fang Li, Rui Zhang, Wen Li, Bin Bin Wang
Publikováno v:
Key Engineering Materials. :586-589
In this study, glassy phase is formed by SiO2-K2O addition to serve as amorphous grain boundary transition layer. SiC (SiO2-K2O) / Cu composite material were prepared by two-step coating method and hot pressing sintered below 770°C, 30MPa for 1.5h,