Publikováno v:
Journal of Korean Foot & Ankle Society. Dec2024, Vol. 28 Issue 4, p119-131. 13p.
Autor:
WS Johnson
Boron/aluminum can develop significant internal matrix cracking when fatigued. These matrix cracks can result in a 40 percent secant modulus loss in some laminates, even when fatigued below the fatigue limit. It is shown that the same amount of fatig
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::cbce61e93a3e792074d9bae8efceb7c4
https://doi.org/10.1520/stp31821s
https://doi.org/10.1520/stp31821s
Autor:
WS Johnson, CA Bigelow
Two specimen configuration of a (0/90)2s SCS-6/Ti-15-3 laminate were tested and analyzed: a center hole (CH) specimen and a double edge notch (DEN) specimen. The two specimen configurations failed at similar stress levels. Two analytical techniques,
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::039608ff93ed89b1ee85e94f8adc58b7
https://doi.org/10.1520/stp24297s
https://doi.org/10.1520/stp24297s
Autor:
S Mall, WS Johnson
The fatigue damage mechanism of an adhesively bonded joint between fabric reinforced composite adherends was investigated with cracked-lap-shear specimens. Two bonded systems were studied: fabric Kevlar 49/5208 epoxy adherends bonded together with ei
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::2b627a3591ab47821c87b917a3ebe2ec
https://doi.org/10.1520/stp30337s
https://doi.org/10.1520/stp30337s
Static and fatigue tests were carried out on two commercial modified epoxy film adhesives with a wide open knit polyester carrier in order to compare crack resistance in mode I and mixed mode I-III loading. The carrier cloth is found to have a signif
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::09a0b3572723d757cee6de56e188d0fc
https://doi.org/10.1520/stp30335s
https://doi.org/10.1520/stp30335s
Autor:
WS Johnson, RA Everett
The repeatability of debond growth rates in adhesively bonded subjected to constant-amplitude cyclic loading was studied. Debond growth rates were compared from two sets of cracked-lap-shear specimens that were fabricated by two different manufacture