Materials Science and Technology. :1-8
In this study, hot workability of Ti–35V–15Cr–0.3Si–0.1C alloy is investigated in the temperature range of 900–1150°C and strain rate range of 0.01–10 s− 1 using processing maps. In the maps, the stability domain displays the feature o
Publikováno v:
Journal of Alloys and Compounds. 631:340-349
The crack initiation behavior and the fatigue limit of Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy with basket-weave microstructure were studied by means of OM, SEM and EDS analysis. Five double annealing processes were conducted to achieve differ
Publikováno v:
Journal of Alloys and Compounds. 603:239-247
The kinetics of static globularization of the hot worked Ti-17 alloy with initial lamellar microstructure was investigated. For this purpose, Ti-17 alloy was isothermally forged to different height reductions at 820 °C or 860 °C and subsequently he
Publikováno v:
Journal of Materials Engineering and Performance. 23:3577-3585
High-temperature deformation behavior tests of as-cast Ti-45Al-2Cr-3Ta-0.5W alloy were conducted over a wide range of strain rates (0.001-1.0 s−1) and temperatures (1150-1300 °C). The flow curves for the current alloy exhibited sharp peaks at low
Publikováno v:
Materials Science and Engineering: A. 598:236-243
The hot deformation behavior of Ti–3Zr–2Sn–3Mo–25Nb (TLM) titanium alloy in the temperature range of 750–850 °C and strain rate range of 0.001−1 s −1 has been investigated by hot compressive testing on the Gleeble-3800 thermal and mech
Publikováno v:
Materials Science and Technology. 31:212-219
The high cycle fatigue (HCF) properties of forged BT25 titanium alloy was examined by fractographic and quantitative microstructural analysis. Two different height reductions (50 and 80%) were applied to the isothermal compression of BT25 alloy with
Publikováno v:
Materials Science and Technology. 30:893-899
Microstructure and properties of different rolling orientation with aging temperature varying in a newly developed Al–Li alloy was investigated by transmission electron microscopy (TEM) analysis. Sheets of experimental Al–Li alloy were solution t
Publikováno v:
Materials Science and Technology. 30:665-669
Ti–3Zr–2Sn–3Mo–25Nb (TLM) titanium alloys are compressed at the 850°C temperature and 0·1 s−1 strain rate. The behaviour of unsteady flow softening with the oscillation of the flow stress–strain curve is observed during hot compression,
Publikováno v:
Journal of Alloys and Compounds. 577:633-642
In this study, both oxidation behavior and tensile properties of Ti–5Al–5Mo–5V–1Cr–1Fe alloy are investigated in air between 100 °C and 1000 °C. X-ray diffraction and light optical microscope are used to characterize the phase composition
Publikováno v:
Proceedings of the 13th World Conference on Titanium
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::22fa14f21bcd8159b087fa642a26a5f1
https://doi.org/10.1002/9781119296126.ch113
https://doi.org/10.1002/9781119296126.ch113