Publikováno v:
International Journal of Fatigue. 100:466-476
Cyclic stress-strain response and fatigue damage character has been investigated in austenitic stainless steel 316L. Hollow cylindrical specimens were cyclically deformed in torsion and combined axial-torsion under constant strain rate condition and
Publikováno v:
Frattura ed Integrità Strutturale, Vol 11, Iss 40 (2017)
Frattura ed Integrità Strutturale; Vol 11 No 40 (2017): April 2017; Pages 162-169
Frattura ed Integrità Strutturale; V. 11 N. 40 (2017): April 2017; Pages 162-169
Frattura ed Integrità Strutturale, Vol 11, Iss 40, Pp 162-169 (2017)
Frattura ed Integrità Strutturale; Vol 11 No 40 (2017): April 2017; Pages 162-169
Frattura ed Integrità Strutturale; V. 11 N. 40 (2017): April 2017; Pages 162-169
Frattura ed Integrità Strutturale, Vol 11, Iss 40, Pp 162-169 (2017)
Cyclic stress-strain response and fatigue damage character has been investigated in austenitic stainless steel 316L. Hollow cylindrical specimens have been cyclically deformed in combined tension-compression and torsion under constant strain rate con
Publikováno v:
Solid State Phenomena. 258:273-276
Thermomechanical fatigue experiments were performed with austenitic stainless Sanicro 25 steel. Several amplitudes of mechanical strain in a wide temperature interval (250-700 °C) were applied to the specimens. Mechanical response was recorded and f
Publikováno v:
Materials Science and Engineering: A. 658:221-228
Evolution of the surface profile in room temperature cyclic loading has been studied in high alloy austenitic Sanicro 25 stainless steel. The localization of the cyclic plastic strain into persistent slip bands in the volume of the material leads to
Publikováno v:
Procedia Structural Integrity. 2016, vol. 2, issue 1, p. 3407-3414.
Superaustenitic stainless steel Sanicro 25 has been subjected to in-phase and out-of-phase thermomechanical fatigue (TMF). Different amplitudes of mechanical strain and the changes of the temperature in the interval 250 to 700°C were applied to stan
Publikováno v:
Materials Science and Engineering: A. 650:52-62
Heat resistant austenitic Sanicro 25 steel was subjected to in-phase and out-of-phase thermomechanical fatigue (TMF) loading conditions with different amplitudes of mechanical strain in a wide interval of temperatures (250–700 °C). Cyclic hardenin
Publikováno v:
Fatigue & Fracture of Engineering Materials & Structures. 38:936-947
The remarkable microstructural stability of high chromium steels prepared by powder metallurgy and strengthened by dispersion of nanometric yttrium oxides in cyclic loading at high temperatures is reported. Contrary to the continuous cyclic softening
Publikováno v:
Materiálové Inžinierstvo, Vol 22, Iss 1, Pp 48-53 (2015)
The influence of the surface preparation of AISI 316L stainless steel by mechanical grinding, polishing and following passivation was examined by immersion corrosion tests in solution simulating body fluids. Decreasing of the surface roughness by fin
Publikováno v:
Materials Science and Engineering: A. 767:138407
Austenitic stainless 316L steel in cold worked condition was subjected to torsional cyclic loading with equivalent strain amplitudes of 0.3% and 0.4% and multiaxial (in-phase and out-of-phase) cyclic loading with equivalent strain amplitude of 0.35%
Publikováno v:
Materiálové Inžinierstvo, Vol 17, Iss 2, Pp 15-19 (2010)
AISI 316Ti is Cr–Ni–Mo austenitic stainless steel with the high Pitting Resistance Equivalent Number (PREN). The effect of the surface finishing by polishing on the pitting corrosion resistance was tested in aggressive 5% FeCl3 solution. The imme