Autor:
V. M. Goritskii, G. R. Shneiderov
Publikováno v:
Russian Metallurgy (Metally). 2021:559-562
The influence of the carbon, zirconium, and vanadium content on the brittle fracture resistance characteristics of 14KhGNDTs weather-resistant steel is studied. The correlation between the ductile crack extension energy and the volume fraction of pea
Autor:
V. M. Goritskii, O. V. Goritskii
Publikováno v:
Metallurgist. 64:1136-1149
Using correlation-regression analysis, the effects of structure and chemical composition on KCV impact strength anisotropy and difference in critical brittleness temperatures for longitudinal and transverse specimens of ferrite-pearlite and high-stre
Publikováno v:
Russian Metallurgy (Metally). 2020:1235-1241
The causes and character of the fracture of a section cut from a main gas pipeline 530 mm in diameter made of low-alloy 17GS steel have been investigated. The length of a longitudinal main crack in the base metal is 12 m. The gas pipeline failed due
Publikováno v:
Metallurgist. 64:425-437
The structure and mechanical properties under tension and impact bending of eleven batches of high-strength manganese-containing steels (Mn-steels) containing 0.09 to 0.14 wt.% Ti subjected to thermomechanical rolling were studied in the temperature
Publikováno v:
Russian Metallurgy (Metally). 2020:461-469
The structure, the static tensile properties, the impact toughness, and the fracture mechanisms of the 12GSB pipe steel specimens cut from the defect regions in a pipeline 530 mm in diameter are studied. Hydrogen corrosion is found to affect the anom
Publikováno v:
Russian Metallurgy (Metally). 2019:1143-1150
—The cause and the mechanism of formation of a long crack in a linear oil-trunk pipeline section consisting of two longitudinal pipes 1220 mm in diameter made of low-alloy 17G1S steel are comprehensively studied. The length of the crack moving alon
Publikováno v:
Metallurgist. 63:21-32
Based on the analysis of the Russian-made 4 to 16 mm thick rolled products produced by thermomechanical rolling from high-strength (yield point: 433 to 828 MPa) low-alloyed welding steels obtained as a result of 15 melting runs, the effect of chemica
Publikováno v:
Russian Metallurgy (Metally). 2019:431-435
The influence of the cold plastic deformation that appear in bending zones and subsequent strain aging on the brittle fracture resistance of galvanized low-carbon steel sheets (2.0–3.0 mm thick) intended for light thin-walled constructions is studi
Publikováno v:
Metallurgist. 62:753-765
Mechanical properties are investigated for tensile and impact bending in longitudinal and transverse Charpy and Menage specimens of Strenx 650 MC and Strenx 700 MC steels, produced by thermomechanical rolling technology. A marked effect is establishe
Autor:
V. M. Goritskii
Publikováno v:
Metallurgist. 62:247-253
The effect of various factors (hydrogenation, segregation of phosphorus, arsenic and other elements), which reduce the cohesive strength of grain boundaries, on the ductile-brittle transition in structural steels is considered. It is shown that durin