Publikováno v:
Strength of Materials. 23:863-869
We have investigated the failure ductility of a 2V-type ductile titanium alloy with a nitrogen and oxygen impurity content ranging from 0.05 to 0.35%. Here we have employed approaches that are based on utilization of the J integral. We have establish
Publikováno v:
Strength of Materials. 23:854-862
We have investigated the effect of nitrogen and oxygen contaminants within a range of concentrations of 0.05–0.35 % on the mechanical properties and crack resistance of a 2V-type ductile titanium alloy. We have demonstrated that the characteristics
Publikováno v:
Strength of Materials. 22:1562-1569
Investigations were carried out into the fatigue crack growth resistance of welded joints in structural titanium alloys contaminated with embrittling impurities. The crack closure effect was taken into account so that it is possible to determine the
Autor:
V. T. Troshchenko, B. T. Timofeev, A. Ya. Varovin, P. V. Yasnii, V. V. Pokrovskii, V. L. Yarusevich, V. V. Zakharchenko
Publikováno v:
Strength of Materials. 20:143-149
The speed of propagation of the fatigue crack at 293 and 623~ and also the characteristics of fracture toughness under static and cyclic loading were investigated under conditions of eccentric tension of compact specimens, 25 mm thick, on a servohydr
Publikováno v:
Strength of Materials. 20:316-320
1. In the welded joints studied according to the results of short-term static tests the basic metal and the heat-affected zone have higher strength and lower ductility than weld metal. 2. A crack in the metal of the heat-affected zone in the test wel