The channel pipes of the control and safety systems of RBMK-1000 reactors are made of a Zr–2.5% Nb (E125) alloy and must operate for 45 years. The evolution of the alloy structure under the action of long-term low-temperature neutron irradiation is
Publikováno v:
Russian Metallurgy (Metally). 2020:799-805
A model is developed to describe the final stage of transient swelling of austenitic steels, at which vacancy pores do not form. The evolution of an ensemble of radiation pores is determined by the following two processes: the growth of vacancy pores
Publikováno v:
Inorganic Materials: Applied Research. 8:370-377
On the basis of the results of X-ray diffraction and microscopy studies of ChS-68 austenitic steel after neutron irradiation at 370°C with doses up to ~2 dpa, a statistical analysis of experimental data was carried out; a linear model of the depende
Autor:
M. S. Lyutikova, V. A. Tsygvintsev, V. S. Shikhalev, S. A. Averin, A. V. Kozlov, E. A. Kinev, V. I. Pastukhov, A. V. Barybin, V. L. Panchenko, N. V. Glushkova, S. V. Barsanova, M. V. Evseev, L. P. Sinel’nikov
Publikováno v:
Atomic Energy. 121:240-248
Data on a shielded-enclosure block, which is part of the scientific-research complex at the Institute of Reactor Materials, are presented. The equipment for the primary post-reactor studies and methods of flaw detection in objects are described. Arti
Autor:
V. L. Panchenko, I. A. Portnykh
Publikováno v:
The Physics of Metals and Metallography. 117:611-623
The phase composition and the characteristics of vacancy voids in cold-worked steel 07C–16Cr–19Ni–2Mo–2Mn–Ti–Si–V–P–B (CW EK164-ID) after neutron irradiation at damaging doses of 36–94 dpa and temperatures of 440–600°C are inve
Publikováno v:
The Physics of Metals and Metallography. 115:625-633
The microstructure of samples of cladding tubes made of steel 0.07C-16Cr-19Ni-2Mo-2Mn-Ti-Si-V-P-B (EK164) irradiated to different damaging doses (up to 77 dpa) in the BN-600 reactor at temperatures from 440 to 600°C has been investigated. Characteri
Publikováno v:
The Physics of Metals and Metallography. 113:520-531
At present, it is the austenitic cold-deformed steel EK164 (06Kh16N20M2G2BTFR)-ID that is considered as a promising material for the achievement of a maximum damage (no less than 110 dpa) and maximum burnup (≥15%). In this work, we have determined
Autor:
E.A. Kinev, Taira Okita, A. V. Kozlov, P. I. Yagovitin, M. V. Evseev, E. N. Shcherbakov, F.A. Garner, Mitsuyuki Sagisaka, Naoto Sekimura, V. L. Panchenko, I. Isobe
Publikováno v:
Journal of Nuclear Materials. :152-156
The results of the examination of the specimens constructed from the Fe–18Cr–9Ni steel thick-wall pipe irradiated at temperatures 370–375 °С to damage rates from 1.5 to 21 dpa at displacement rates from 3 × 10 −9 to 4 × 10 −8 dpa/s are
Publikováno v:
Journal of Nuclear Materials. :925-929
Argon-pressurized tubes of 20% cold-worked 16Cr15Ni2MoTiMnSi steel were irradiated at hoop stresses of 0, 100 and 200 MPa at ∼740 K in the BN-600 fast reactor to 108 dpa. Following nondestructive measurements of strain, density measurements and mic
Autor:
L. A. Skryabin, A. V. Nikulina, L. P. Sinel’nikov, V. A. Tsygvintsev, V. L. Panchenko, V. N. Shishov, V. E. Kalachikov, S. A. Averin
Publikováno v:
Metal Science and Heat Treatment. 45:304-308
Variation of the phase composition and structure of zirconium alloys E125 and E635 under the action of irradiation is studied by the methods of microscopic x-ray energy dispersion analysis, radiographic analysis, and analytical transmission electron