Zobrazeno 1 - 10
of 14
pro vyhledávání: '"V. I. Breus"'
Analysis of the Hydraulic Regimes of Vertical Waste-Heat Boilers of Combined-Cycle Gas-Turbine Units
Publikováno v:
Power Technology and Engineering. 53:466-472
An analysis of the hydraulic system of the natural circulation loop of the waste-heat boilers of combined-cycle gas turbine units is performed. It is demonstrated that the standard method of hydraulic calculation of steam boilers based on an evaluati
Publikováno v:
Power Technology and Engineering. 53:78-83
An analysis of the causes of erosion-induced wear of the metal in pipe bends of evaporator heating pipe surfaces is performed based on experience gained from the operation of the heat-recovery boilers of combined-cycle (steam-gas) power plants. Damag
Autor:
N. S. Shestakov, K. Y. Ogonkov, V. A. Ageev, O. A. Korzhikova, S. P. Tupitsyn, G. F. Chebakova, V. I. Breus, K. A. Grigoryev, A. P. Sorokin, A. E. Leikam
Publikováno v:
Safety and Reliability of Power Industry. 10:291-297
The article presents modern burner devices for power and industrial boilers that provide NOx emissions (when burning natural gas — 125 mg/m3, when burning fuel oil — 250 mg/m3). The burners are equipped with modern ignition safety devices and inj
Autor:
O. L. Anisimova, A. B. Barannikov, V. I. Breus, V. N. Tambovtseva, V. F. Petukhova, A. P. Musikov
Publikováno v:
Power Technology and Engineering. 47:362-366
The drum internals and the internal arrangement of BKZ-75-39FB steam boiler were modified to improve the quality of steam to comply with the ratings of MAN Turbo AG MARC4-CO1 turbine. The commissioning tests of separators confirmed the decisions made
Publikováno v:
Power Technology and Engineering. 47:133-138
Calculations show that to prevent the oscillatory instability of the flow in a PK-47 once-through boiler, it is necessary to install /12 mm orifice plates at the inlet of its bottom radiant section. Load-reduction tests on the boiler with such plates
Publikováno v:
Thermal Engineering. 59:421-424
Design solutions worked out for the main equipment of coal-fired power units for ultrasupercritical initial steam conditions are reviewed.
Publikováno v:
Thermal Engineering. 59:183-188
Results from work on analyzing the performance of the P-90 heat-recovery boilers used as part of the PGU-450T-based Unit 1 at the Severozapadnaya cogeneration station and on revealing factors causing damage to the bends of evaporating tubes are prese
Autor:
V. I. Breus, I. I. Belyakov
Publikováno v:
Thermal Engineering. 57:612-616
Results of research works on studying the occurrence of hydraulic instability in once-through boilers in startup modes and during operation at sliding pressure are presented. To prevent the occurrence of hydraulic instability, it is suggested that th
Publikováno v:
Thermal Engineering. 56:124-128
The results of investigation into the nature of damage to tube bends of the low-pressure evaporator of the P-90 heat recovery boiler installed at the Severozapadnaya cogeneration plant are presented. It has been found that damage was caused by cavita
Publikováno v:
Power Technology and Engineering. 42:344-348
The causes of damage to the baffle pipes in BKZ-420-140PT-2 high-pressure drum boilers during combustion of Irsha-Borodin and Zheronskii coals are analyzed. Damage to the salt module pipes was caused by the buildup of internal sediments and untimely