Zobrazeno 1 - 5
of 5
pro vyhledávání: '"V. G. Chernichenko"'
Autor:
V. A. Lutsenko, V. G. Chernichenko, I. V. Sikachina, T. N. Golubenko, O. V. Lutsenko, K. Yu. Kluchnikov
Publikováno v:
Litʹë i Metallurgiâ, Vol 0, Iss 4, Pp 92-96 (2012)
The nontraditional technology of scale removal from the high-carbon wire surface by means of mechanical scalebreaking with electrolyte-plasma post-treatment is developed and tested.
Externí odkaz:
https://doaj.org/article/8455281a1ae54b529a32e265a42308a8
Publikováno v:
Litʹë i Metallurgiâ, Vol 0, Iss 4, Pp 57-59 (2012)
It is shown that at twisting of wire of diameter 1,83 mm, produced by direct wire drawing of thermomechanically processed rolled wire of diameter 5,5 mm of steel 90, metal stratification is completely eliminated at decrease of carbon, manganese and a
Externí odkaz:
https://doaj.org/article/60554d51b28a42f0965a6e19505ee6ff
Publikováno v:
Litʹë i Metallurgiâ, Vol 0, Iss 4, Pp 102-104 (2011)
It is shown that at twisting of wire of diameter 1,83 mm, produced by direct wire drawing of thermomechanically processed rolled wire of diameter 5,5 mm of steel 90, metal stratification is completely eliminated at decrease of carbon, manganese and a
Externí odkaz:
https://doaj.org/article/0ddd7d5e6d6b4f36838fca177919a797
Publikováno v:
Steel in Translation. 40:853-856
Kinetic data on austenite decomposition in high-carbon alloy steel in the continuous cooling of wire rod permit the determination of the best thermomechanical treatment. Regulation of the chemical composition of the steel (the carbon, chromium, and m
Publikováno v:
Steel in Translation. 42:794-796
In twist tests of high-tension bronzed wire (diameter 1.55–1.83 mm) produced by direct drawing from thermomechanically treated wire rod (diameter 5.5 mm), lamination of the metal may be completely eliminated if the carbon and manganese content is r