Zobrazeno 1 - 10
of 26
pro vyhledávání: '"V. D. Frechette"'
Boron Oxide plays a key role in numerous glasses of high technological importance, yet its role in glass structure is far from clear. Indeed, in recent years there have been serious chal lenges to previous structure concepts for both crystalline an
Autor:
V. D. Frechette
Quality Assurance in Ceramic Industries represents the proceedings of a conference held at the New York State College of Ceramics, Alfred University, June 4-7, 1978, as fifteenth in a continuing series rotated annually among Alfred University, North
Publikováno v:
Journal of the American Ceramic Society. 73:43-48
Electrical de fields applied through electrodes on either side of a slow-running crack in soda-lime-silica glass resulted in a deviation of the crack plane and in delayed deceleration, arrest, and healing. In some cases crack closure occurred while s
Autor:
V. D. Frechette, Mary Kay Clark Holden
Publikováno v:
Journal of the American Ceramic Society. 72:2189-2193
Chill checks of controlled depth were produced in soda-lime-silica glass, and an optimum humidity of 30 kPa (300 mbar) water vapor pressure was found to heal these checks in an annealing cycle. Critical factors were found to be a fluxing effect, havi
Autor:
V. D. Frechette, M. P. Singh
Publikováno v:
Finite Elements in Analysis and Design. 6:81-95
The finite element technique was used to trace the sequence of bond breakages in a precracked ideal MgO crystal under dynamic loading. The crack velocity was then calculated from the time interval between the breaking of successive bonds. There was a
Publikováno v:
Journal of the American Ceramic Society. 64:463-468
Thin films of gold were deposited by evaporation onto glass surfaces generated by slow fracture in a vacuum. Such films characteristically show an agglomerated or coalesced structure. Deliberate contamination of the substrate and growing films with O
Autor:
Terry A. Michalske, V. D. Frechette
Publikováno v:
Journal of the American Ceramic Society. 63:603-609
Crack growth in glass plates, up to supercritical velocities, was produced by controlled strain, velocity being measured continuously by superimposing a tuned-frequency sonic signal during cracking. Cracks, which were accelerated to supercritical vel
Autor:
V. D. Frechette, H. J. Oel
Publikováno v:
Journal of the American Ceramic Society. 69:342-346
Stress distributions calculated for thin disks having a cylindrical inclusion were found to agree with those measured for glass specimens cooled to room temperature after they were sealed. Maximum circumferential stress in the sheath was independent
Autor:
C. L. Quackenbush, V. D. Frechette
Publikováno v:
Journal of the American Ceramic Society. 61:402-406