Publikováno v:
Journal of Applied Spectroscopy. 55:1024-1028
Publikováno v:
Refractories. 32:83-86
New and effective refractories have been developed whose physicotechnical and working parameters are better than those of existing Soviet and foreign materials. Commercial production of them has been organized. MKFU-83 and KKFU-76 refractories increa
Publikováno v:
Journal of Applied Spectroscopy. 57:640-642
Autor:
V. A. Chernyakhovskii
Publikováno v:
Refractories. 26:41-44
The method of production of periclase-spinel parts with a phosphate binder provides high physicotechnical properties in them and does not require high temperature firing. The unfired parts may be used for lining the burning zone of rotating cement an
Autor:
A. P. Dubrovin, L. I. Krigman, M. D. Karaseva, V. A. Chernyakhovskii, S. I. Ivashchenko, M. A. Rabinovich
Publikováno v:
Refractories. 15:610-613
Phosphate binder in the form of orthophosphoric acid or alumino—chromo—phosphate binder gives a strong material over the firing temperature range 700–1000°C while standard corundum brick must be fired at 1750°C to achieve the same strength.
Autor:
V. A. Chernyakhovskii, V. K. Vorob'ev
Publikováno v:
Refractories. 28:461-464
Autor:
V. A. Chernyakhovskii, V. K. Vorob'ev
Publikováno v:
Refractories. 28:195-201
The relative effect of the parameters on the properties of the vibratory compacted specimens decreases in the following order: the moisture content of the body, the content of the finely milled fraction, the static pressure, the duration of applicati
Autor:
V. A. Chernyakhovskii, L. M. Krigman, M. A. Rabinovich, I. V. Grigor'ev, M. D. Karaseva, V. A. Kopeikin, S. I. Ivashchenko
Publikováno v:
Refractories. 18:169-174
The composition was developed for a corundum refractory, the characteristics (other than the chemical and mineral compositions) and metal resistance of which are on the level of those of an imported tested refractory.
Publikováno v:
Refractories. 29:538-543
A thermal shock resistant corundum refractory was developed using a phosphate binder (TU 14-8-511-86). This refractory is recommended for protecting various thermal units against the action of molten metals, slags, sodium sulfide, and mechanical and
Publikováno v:
Refractories. 16:377-379
The binders AChPhB-E and AChPhB-T can be used for producing ladle brick in the same way as standard AChPhB binder. An increase in the proportion of binder, regardless of the type, helps to increase the thermal and mechanical strength and to reduce th