Zobrazeno 1 - 10
of 47
pro vyhledávání: '"Tapio Saukkonen"'
Publikováno v:
Corrosion Reviews. 36:281-293
The selective dissolution of ferrite phase from the pearlite was studied in fuel-grade ethanol (FGE) to understand how it affects the stress corrosion cracking (SCC) mechanism of carbon steel in FGE. It was shown that microgalvanic coupling occurs be
Publikováno v:
Toivonen, A, Hänninen, H, Saukkonen, T & Aaltonen, P 2017, ' Environmentally assisted cracking crack initiation in nickel-based alloy dissimilar metal welds in doped and pure steam and pressurized water reactor water ', Corrosion, vol. 73, no. 7, pp. 808-821 . https://doi.org/10.5006/2339
Environmentally assisted cracking (EAC) susceptibilities of Alloys 600, 690, and their weld metals with and without weld defects were benchmarked in pure and doped hydrogenated steam at 400°C and pressurized water reactor (PWR) water at 360°C on fo
Autor:
Filip Tuomisto, Pertti Aaltonen, Simo Kilpeläinen, Yuriy Yagodzinskyy, Tapio Saukkonen, Hannu Hänninen
Publikováno v:
Corrosion Reviews. 33:487-500
The role of the excessive metal vacancy generation in transgranular stress corrosion cracking (TGSCC) of pure copper was studied in relation to crack initiation and growth mechanisms. Electrochemically polarized specimens were strained at room temper
Autor:
Yuriy Yagodzinskyy, Hannu Hänninen, Tapio Saukkonen, Olga Todoshchenko, Valentina Yagodzinska
Publikováno v:
Corrosion Reviews. 33:515-527
Constant load tests of high-strength carbon steels with different micro-alloying using strengths in the range of 1000–1400 MPa were performed at ambient temperature under continuous electrochemical hydrogen charging. Hydrogen markedly affects delay
Publikováno v:
Corrosion Science. 96:14-22
The intrinsic dissolution rate of manganese sulfide (MnS) was measured in water with hydrochloric acid and in fuel-grade ethanol (FGE) with acetic acid and hydrochloric acid using static disk system. The intrinsic dissolution rate of MnS is used to e
Publikováno v:
ISIJ International. 55:2182-2188
VK: T20309
Autor:
Mikko Heikkilä, Pekka Pohjanne, Thomas Ohligschläger, Isto Virtanen, Tapio Saukkonen, Martti Pulliainen, Konsta Sipilä, Carl-Gustav Berg, Timo Saario, Juha Koskiniemi, Jyrki Romu, Hannu Hänninen, Mikko Vepsäläinen
Publikováno v:
Pohjanne, P, Vepsäläinen, M, Saario, T, Sipilä, K, Romu, J, Saukkonen, T, Hänninen, H, Heikkilä, M, Koskiniemi, J, Berg, C-G, Pulliainen, M, Virtanen, I & Ohligschläger, T 2015, ' Effect of Electrochemical Potential on Stress Corrosion Cracking Susceptibility of EN 1.4301 (AISI 304) Austenitic Stainless Steels in Simulated Hot Black Liquor ', Corrosion, vol. 71, no. 7, pp. 887-894 . https://doi.org/10.5006/1594
Stress corrosion cracking (SCC) susceptibility of austenitic EN 1.4301 (AISI 304, UNS S30400) stainless steel was studied as a function of electrode potential at T = 190°C in 15 g/kg NaOH + 150 g/kg Na2S containing caustic environment simulating hea
Autor:
Sami Jouttijärvi, Jyrki Romu, Janne Halme, Jarkko Etula, Tapio Saukkonen, Peter Lund, Kati Miettunen
Publikováno v:
Progress in Photovoltaics: Research and Applications. 23:1045-1056
The main issue in using low cost metals in dye solar cells is the corrosion caused by the liquid electrolyte. Contrary to typical applications of metals, the adverse effects of corrosion in dye solar cells are related to irreversible depletion of cha
Publikováno v:
Metallurgical and Materials Transactions A. 45:4742-4747
High-strength carbon steels of 1200 MPa strength level with different microalloying were tensile tested at constant extension rate and constant load under continuous electrochemical hydrogen charging. The results show that hydrogen markedly reduces e
Publikováno v:
Materials and Corrosion. 66:95-104
Grain boundary engineering (GBE) of 304 and 316 austenitic stainless steels has been widely researched but studies on other grades of austenitic stainless steels are less common. In this study, application of GBE on metastable austenitic stainless st