Zobrazeno 1 - 10
of 24
pro vyhledávání: '"Taku Arai"'
Autor:
Taku Arai
Publikováno v:
Journal of the Atomic Energy Society of Japan. 61:100-102
Autor:
Toshiari Saegusa, Taku Arai
Publikováno v:
Basics of Transport and Storage of Radioactive Materials
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::87523a2cd39ee4f7ff5e6e1f587c115e
https://doi.org/10.1142/9789813234048_0008
https://doi.org/10.1142/9789813234048_0008
Publikováno v:
The Proceedings of the Materials and Mechanics Conference. 2015:OS0902-33
Publikováno v:
Volume 1A: Codes and Standards.
In this study, CASSs which were thermally aged at 275–400°C for up to 30000 hrs were investigated using atom probe tomography, Charpy impact test, hardness test, and fracture toughness test in order to evaluate the effects of chemical composition
Autor:
Taku Arai, Yasufumi Miura
Publikováno v:
The Proceedings of the Materials and Mechanics Conference. 2019:OS1316
Publikováno v:
Nuclear Engineering and Design. 238:1227-1232
Susceptibility to chloride induced stress corrosion cracking (ESCC) of candidate canister materials, UNS S31260 and UNS S31254 stainless steels (SS), was investigated by a constant load test in air at temperatures of 343 and 353 K with relative humid
Publikováno v:
Zairyo-to-Kankyo. 56:93-98
Publikováno v:
MATERIALS TRANSACTIONS. 48:1431-1437
Chloride-induced stress corrosion crack growth rates were measured for candidate canister materials in a simulated marine atmospheric environment. Half-inch compact tension specimens were used to obtain stress corrosion crack growth rates by applying
Publikováno v:
Volume 1A: Codes and Standards.
The JSME Codes and Standards Committee have provided many kinds of crack growth rates of SCC and fatigue cracking as Appendix in the code and the code cases. However each code has been separately investigated and there is no common rule among SCC gro
Publikováno v:
Zairyo-to-Kankyo. 55:20-24