Publikováno v:
Fusion Engineering and Design. 135:204-215
Oxidation behaviour of Reduced Activation Ferritic Martensitic Steel (RAFMS), the structural material for fusion reactors, exposed to atmosphere for ∼2 years has been studied giving special emphasis on the morphology and chemistry of the oxides for
Autor:
P. Chandramohan, Sinu Chandran, Veena Subramanian, T.V. Krishnamohan, Tom Mathews, Raghavendra Y, M.P. Srinivasan, H. Subramanian
Publikováno v:
Journal of Nuclear Materials. 553:153043
Inorganic metal ion additives are being explored for controlling the corrosion and deposition of activated corrosion products on out of core surfaces in Pressurized Heavy Water Reactors (PHWRs). Mg2+ ions can modify the oxides on heat transfer surfac
Autor:
D. Mohan, Sinu Chandran, S. Rangarajan, Puspalata Rajesh, Sankaralingam Velmurugan, Padma S. Kumar
Publikováno v:
Materials Chemistry and Physics. 187:18-27
Materials undergo enhanced corrosion in the presence of oxidants in aqueous media. Usually, hydrogen gas or water soluble reducing agents are used for inhibiting corrosion. In the present study, the feasibility of using alternate reducing agents such
Autor:
P. Chandramohan, Veena Subramanian, Santanu Bera, H. Subramanian, Sinu Chandran, S.V. Narasimhan, S. Rangarajan
Publikováno v:
Materials Chemistry and Physics. 145:499-509
Flow accelerated corrosion leads to wall thinning of outlet-feeder pipes in the primary heat transport system of pressurized heavy water reactors and can even necessitate enmasse feeder replacement. Replacement of carbon steel 106-grade-B (CS) with c
Publikováno v:
Journal of Applied Electrochemistry. 39:1617-1623
The dissolution behaviour of stellite #3 in two oxidizing agents of equivalent acidity namely, permanganic acid (HMnO4) and a mixture of nitric acid and potassium permanganate (NP) was evaluated. The presence of nitrate in the permanganate formulatio
Autor:
Sriram Narasimhan, H. Subramanian, Sumathi Suresh, Sinu Chandran, Sankaralingam Velmurugan, Puspalata Rajesh, Padma S. Kumar
Publikováno v:
Corrosion Engineering, Science and Technology. 42:174-182
Type 304 stainless steel and carbon steel are extensively used as structural materials in the reactor coolant systems of nuclear power plants. The corrosion of these structural materials during normal operation and the subsequent neutron activation o
Autor:
Sankaralingam Velmurugan, Sinu Chandran, Shaju K. Albert, S.V. Narasimhan, S. Rangarajan, V. Ramasubbu, S. Navin Vinayak, Veena Subramanian
Publikováno v:
International Journal of Nuclear Energy Science and Technology. 6:199
In the moderator system of some nuclear power plants, subsequent to the activation of the safety shutdown system, Gd 3+ is removed by ion exchange prior to reactor start-up. During this process, the pH of the system water can get lowered to 3 due to