Zobrazeno 1 - 10
of 345
pro vyhledávání: '"Sinterización"'
Publikováno v:
Boletín de la Sociedad Española de Cerámica y Vidrio, Vol 62, Iss 2, Pp 194-202 (2023)
Tin oxide is one of the most extensively studied semiconductor materials due to its broad field of applications. On the one hand, its high conductivity and its corrosion resistance are the most remarkable properties. Therefore, one of the most develo
Externí odkaz:
https://doaj.org/article/6f7f3fe8caa8466599a6ad1e37f80a96
Autor:
Yassine Et-Tayea, Achraf Harrati, Ahmed Rachid, Hicham Nasri, Ahmed Attou, Youssef Arkame, Ahmed Manni, Younes Mamouch, Abdeslam El Bouari, Faiçal El Khazanti, Chaouki Sadik
Publikováno v:
Boletín de la Sociedad Española de Cerámica y Vidrio, Vol 62, Iss 3, Pp 268-283 (2023)
The Oued Zemmour deposit is associated to Neogene volcanism in the Kert basin, Nador area (Morocco), and thus one of the numerous bentonite occurrences in the Gourougou volcano's region. To assess their potential use, this article examines the Oued Z
Externí odkaz:
https://doaj.org/article/066be8e673cf41d7a3ecbf2c6b3cf24c
Publikováno v:
Anuario de Arqueología, Vol 15, Iss 15 (2023)
La trascendencia del desarrollo de los procesos tecnológicos alcanzados durante varios miles de años por los orfebres precolombinos radica en el alto desempeño de sus técnicas metalúrgicas, sin conocerse hasta la actualidad, todos los métodos q
Externí odkaz:
https://doaj.org/article/7656d6a3cf6343719d40df18d539d4ac
Publikováno v:
Boletín de la Sociedad Española de Cerámica y Vidrio, Vol 62, Iss 1, Pp 26-39 (2023)
The sintering behaviour of a pyrophyllite clay has been investigated. The mineralogical composition by X-ray diffraction (XRD) of this sample was ∼35 wt.% pyrophyllite, ∼25 wt.% sericite/illite, ∼15 wt.% kaolinite and ∼20 wt.% quartz. The che
Externí odkaz:
https://doaj.org/article/749cbf7fc4584eb59a9aa8ec5395f85b
Autor:
Milica V. Vasić, Lato Pezo, Miloš R. Vasić, Nevenka Mijatović, Miodrag Mitrić, Zagorka Radojević
Publikováno v:
Boletín de la Sociedad Española de Cerámica y Vidrio, Vol 61, Iss 3, Pp 241-251 (2022)
This study presents the 51 mixtures of ceramic clays characterized by using XRF, XRD, granulometry, and dilatometry analyses. After firing in a 1000–1250 °C range, water absorption (WA) according to EN standards by boiling in water, under vacuum,
Externí odkaz:
https://doaj.org/article/573719d1e1114e63a40f68060030f6a5
[ES] Las aleaciones biomédicas de alta entropía (Bio-HEA) con propiedades no tóxicas, sintetizadas mediante métodos de pulvimetalurgia, han recibido una atención limitada a pesar de su potencial para un rendimiento mecánico y biológico favorab
Externí odkaz:
http://hdl.handle.net/10251/208235
Publikováno v:
Boletín de la Sociedad Española de Cerámica y Vidrio, Vol 60, Iss 5, Pp 307-317 (2021)
Ceramic Injection Moulding (CIM) is an advanced powder processing technology launched three decades ago which has become a growing attractive alternative for new technical applications, such as thermal management and wireless charging. Porcelain-type
Externí odkaz:
https://doaj.org/article/bab2a276f4364eb4a9b124ce387542c8
Publikováno v:
Boletín de la Sociedad Española de Cerámica y Vidrio, Vol 60, Iss 1, Pp 53-61 (2021)
Aluminum-doped zinc oxide (AZO) electrodes can be a good alternative to replace the expensive electrodes (Ti, ITO, FTO, etc.), which are used in the electrooxidation process to remove refractory and emergent contaminants from industrial wastewaters.
Externí odkaz:
https://doaj.org/article/7be00fabd3b44cfebaad8fd01f4c9153
Autor:
Uğur Çavdar
Publikováno v:
Revista de Metalurgia, Vol 57, Iss 1, Pp e188-e188 (2021)
En este trabajo, se estudiaron compuestos de nanoplaquetas de grafeno (GNP) como refuerzo de una aleación de aluminio, estudiándose refuerzos con adiciones variables de hasta un 2,0% en peso de GNP. Los polvos, de diferentes composiciones, se agita
Externí odkaz:
https://doaj.org/article/be822dd06e134f55aa54e2abfca26755
Autor:
Tanju Teker, S. Osman Yilmaz
Publikováno v:
Revista de Metalurgia, Vol 56, Iss 4, Pp e178-e178 (2020)
La mezcla de polvo de Ti+Ni3Al+Al2O3 a base de Fe se alea mecánicamente en un molino de bolas Spex. Los compuestos con adición de Ti+Ni3Al+Al2O3 a base de Fe se produjeron a una temperatura de sinterización de 1000 °C durante un tiempo de 1 h. La
Externí odkaz:
https://doaj.org/article/be20bd085706440d8f5467862dcb30a5