Zobrazeno 1 - 10
of 99
pro vyhledávání: '"Sinha TK"'
Publikováno v:
Clinical Ophthalmology, Vol Volume 18, Pp 1819-1828 (2024)
Debdulal Chakraborty,1 Subhendu Boral,1 Tushar Kanti Sinha,1 Arnab Das,1 Angshuman Mukherjee,1 Saptorshi Majumdar,1 Ranabir Bhattacharya,2 Ritobroto Maitra3 1Department of Vitreoretinal Services, Disha Eye Hospitals, Kolkata, West Bengal, India; 2Dep
Externí odkaz:
https://doaj.org/article/055f756858e742eda516660606c4abff
Publikováno v:
Clinical Ophthalmology, Vol Volume 17, Pp 1067-1076 (2023)
Debdulal Chakraborty,1 Soumen Mondal,1 Subhendu Boral,1 Arnab Das,1 Tushar Kanti Sinha,1 Saptorshi Majumdar,1 Ranabir Bhattacharya,2 Ritobroto Maitra3 1Department of Vitreoretinal Services, Disha Eye Hospitals, Kolkata, West Bengal, India; 2Departmen
Externí odkaz:
https://doaj.org/article/c53c564a7d974ecf810fd37581f5172b
Publikováno v:
Clinical Ophthalmology, Vol Volume 16, Pp 4303-4313 (2022)
Debdulal Chakraborty,1 Aniruddha Maiti,2 Jay U Sheth,3 Soumen Mondal,1 Subhendu Boral,1 Krishnendu Nandi,4 Tushar Kanti Sinha,1 Arnab Das1 1Department of Vitreoretinal Services, Disha Eye Hospitals, Kolkata, West Bengal, India; 2Department of Vitreor
Externí odkaz:
https://doaj.org/article/47f5b5261bfb4a7f9dfe16bad21ef6c0
Publikováno v:
IndraStra Global.
Zr-2.5 wt % Nb alloy sheet, obtained by unfolding and straightening a pressure tube, was further cold rolled upto 39% reduction in thickness to investigate the effect of cold working on the stress (sigma)-strain rate (epsilon)over dot behaviour over
Publikováno v:
IndraStra Global.
Tensile samples of a modified 9Cr-1Mo steel after tempering at 823 and 983 K subsequent to a normalizing treatment at 1373 K (designated as 550T and 710T, respectively) were deformed in tension at temperatures in the range of 77 to 373 K both by cons
Publikováno v:
IndraStra Global.
Samples of Zr-2.5 wt.% Nb alloy, obtained from pressure tube, were annealed in the temperature range 700-900 degrees C up to 100 h to investigate the grain growth behaviour. The grain size increases with annealing time (t) and temperature (T) accordi
Publikováno v:
IndraStra Global.
Tensile testing of a modified 9Cr-.1Mo steel in two microstructural conditions (710T - normalized at 1100 degrees C, tempered at 710 degrees C, and 550T - normalized at 1100 degrees C tempered at 550 degrees C) in the temperature range 25-450 degrees
Publikováno v:
IndraStra Global.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.