M. Utama, M. Suhartini, Herwinarni, Siswanto, S. Yoharmus, H. Sundaru, H.M. Halik, Prayitno, H.M. Muklis, S. Ruslim
Publikováno v:
Atom Indonesia, Vol 31, Iss 2, Pp 61-78 (2005)
One hundred and fifty kg natural rubber latex (NRL) before and after concentration were added with 3 phr (part hundred ratio of rubber) normal butyl acrylate, then the mixture were irradiated at 25 kGy by gamma rays of 60Co in pilot scale. The irradi
Externí odkaz:
https://doaj.org/article/a5908451aff34f309c5b86b1ba314425
Publikováno v:
Atom Indonesia, Vol 31, Iss 2, Pp 79-90 (2005)
Trial production of surgical gloves from irradiated natural rubber latex at the PT. Laxindo Utama Serang Banten glove factory has been carried out. The variation of heating temperature and leaching time during processing were evaluated. The physical
Externí odkaz:
https://doaj.org/article/2efb12422dff4963b64ab7df8190375d
Autor:
Siswanto Siswanto, Suharyanto Suharyanto, Marga Utama, Made Sumarti, S. Ruslim, Herwinarni Herwinarni
Publikováno v:
Atom Indonesia, Vol 31, Iss 2, Pp 79-90 (2005)
Trial production of surgical gloves from irradiated natural rubber latex at the PT. Laxindo Utama Serang Banten glove factory has been carried out. The variation of heating temperature and leaching time during processing were evaluated. The physical
Autor:
Prayitno Prayitno, S. Yoharmus, H. M. Muklis, S. Ruslim, Meri Suhartini, H.M. Halik, Herwinarni Herwinarni, Marga Utama, Siswanto Siswanto, H. Sundaru
Publikováno v:
Atom Indonesia, Vol 31, Iss 2, Pp 61-78 (2005)
One hundred and fifty kg natural rubber latex (NRL) before and after concentration were added with 3 phr (part hundred ratio of rubber) normal butyl acrylate, then the mixture were irradiated at 25 kGy by gamma rays of 60 Co in pilot scale. The irrad