Zobrazeno 1 - 8
of 8
pro vyhledávání: '"S. L. Barbot'ko"'
Publikováno v:
Polymer Science Series D. 9:431-436
Ways to decrease the flammability of rubber materials based on organosilicon rubbers of different structures and on ethylene–propylene–diene rubbers are shown. Data on the influence of the structure of organosilicon rubbers on their flammability
Publikováno v:
Polymer Science Series D. 9:298-302
This paper presents a composition developed for use both as a film adhesive with a working temperature up to 150°C and as a binder for production of fiberglass with a working temperature up to 120°C. The composition is autoextinguishing and contain
Publikováno v:
Polymer Science Series D. 8:110-112
This paper presents the results of investigating the structure, the combustibility, and the basic physical and mechanical properties of sealing ethylene-propylene-diene monomer rubber specimens filled with flame retardants such as aluminum and magnes
Autor:
E. L. Mitina, S. L. Barbot’ko
Publikováno v:
Polymer Science Series D. 5:296-299
The results of investigations of the influence of fire retardants on the combustibility and elastic-strength properties of light-colored resins based on a combination of butadiene-styrene and butadiene rubber are presented. The amounts of fire retard
Autor:
S. L. Barbot’ko
Publikováno v:
Russian Journal of General Chemistry. 81:1068-1074
Influence of various fire-retardant additives, as well as thermostability and chemical structure on polymer flammability is analyzed, and nonfire-resistant and fire-resistant polymer materials are compared. An essential influence of these factors on
Autor:
G. N. Petrova, V. P. Chebotarev, N. S. Yukin, E. Ya. Beider, S. L. Barbot'ko, L. M. Bolotina, S. V. Malyshenok
Publikováno v:
International Polymer Science and Technology. 32:55-59
Publikováno v:
Polymer Science. Series D. 2:31-33
The combustibility of glass and carbon plastics has been studied. It was proven that the value of traceable combustibility indices depend not only on the duration of the sample’s exposure to the burner flame, but also on the thickness of the sample
Publikováno v:
Proceedings of VIAM. :9-9