SiAl enriched Fe based sheets by chemical vapour deposition: Evolution of magnetoelastic properties
Publikováno v:
Journal of Magnetism and Magnetic Materials. 161:292-298
The increase of the Si and A1 concentration in pure Fe, non-oriented and grain-oriented Fe based laminations is expected to produce two fundamental consequences on their general magnetic behavior: decreased magnetoelastic sensitivity and decreased en
Publikováno v:
Journal of Alloys and Compounds. :568-571
With a high silicon content, silicon steel has good soft magnetic properties because of the decreased magnetic anisotropy, lower magnetostriction and higher resistivity. However, above 3.5 wt.% Si a lower ductility makes conventional processing into
Publikováno v:
Journal of Magnetism and Magnetic Materials. 133:205-208
Pure iron sheets were siliconized and aluminized by pack cementation in the temperature range 850–1000°C. Diffusion coatings of Fe-Si-Al solid solution were obtained with concentration gradients. The magnetomechanical damping evolution of enriched
Autor:
Massimo Pasquale, Fausto Fiorillo, Enzo Ferrara, J. Degauque, S. Crottier-Combe, S. Audisio, J.L. Porteseil
Publikováno v:
Journal of Magnetism and Magnetic Materials. 160:151-153
Copyright (c) 1996 Elsevier Science B.V. All rights reserved. Grain-oriented Fe−Si alloys have been Si enriched up to 6.5 wt by a chemical vapour deposition method using SiCl 4 . Both longitudinally and transversally cut laminations exhibit a decre
Autor:
J. Degauque, Marcello Baricco, J.L. Porteseil, S. Audisio, S. Crottier-Combe, C. Beraud, Fausto Fiorillo
Publikováno v:
Journal de Physique IV Proceedings
Journal de Physique IV Proceedings, EDP Sciences, 1995, 05 (C5), pp.C5-1045-C5-1052. ⟨10.1051/jphyscol:19955123⟩
Journal de Physique IV Proceedings, EDP Sciences, 1995, 05 (C5), pp.C5-1045-C5-1052. ⟨10.1051/jphyscol:19955123⟩
Non-oriented and grain-oriented 6.5% Si-Fe laminations have been prepared by means of the dynamic Chemical Vapour Deposition technique, exploiting a chemical reaction at 1000°C between a flowing SiCl 4 + Ar mixture and an iron-silicon based substrat
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::e259d1904f71ee3a047c78ef99dea541
https://hal.archives-ouvertes.fr/jpa-00253795/document
https://hal.archives-ouvertes.fr/jpa-00253795/document
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Publikováno v:
Materials & Corrosion / Werkstoffe und Korrosion; Apr2019, Vol. 70 Issue 4, p593-604, 12p