Zobrazeno 1 - 10
of 131
pro vyhledávání: '"R.K. Shiue"'
Publikováno v:
Key Engineering Materials. 803:8-12
Dissimilar tungsten inert gas (TIG) welding of furnace tube alloys, T92, T91 and T22, using TG-S2CM, TG-S2CW and TG-S9Cb fillers is performed in the experiment. Post weld heat treatments (PWHTs) of specimens selected from wire cutting of the qualifie
Publikováno v:
Key Engineering Materials. 735:49-53
Microstructures, Vickers depth profiles and low-temperature toughness of the tempered direct water quenched steels have been evaluated in the experiment. Martensite dominates the direct quenched specimen, and it is brittle at low-temperature toughnes
Publikováno v:
Key Engineering Materials. 732:55-58
The purpose of this investigation is focused on the direct quench and temper mechanisms of the high strength offshore steel. Microstructural analyses of martensite and retained austenite in the direct quenched steel, simulations of martensitic transf
Publikováno v:
Metallurgical and Materials Transactions A. 47:4777-4783
This study investigates low-temperature toughness of the offshore steel with two different austempering heat treatments. Toughness of upper bainite is significantly lower than that of lower bainite. Low impact toughness of the upper bainite is caused
Publikováno v:
Materials Science and Engineering: A. 653:139-146
A CO 2 laser was applied for dissimilar welding of Ti–15V–3Cr–3Al–3Sn (Ti–15–3) to Ti–6Al–4V (Ti–6–4) alloys. The microstructures and notched tensile strength (NTS) of the dissimilar welds were investigated in the as-welded and po
Publikováno v:
Materials Research Innovations. 19:S10-249
Evaluating vacuum brazed IN-800/VZ-2177/IN-800 joints by changing the brazing parameters was performed. The joint contains two intermetallic phases, B2Cr5P and Cr4Ni3P4, in the Ni-rich matrix. The quantity of Cr4Ni3P4 compound in brazed joint is redu
Publikováno v:
Materials Research Innovations. 19:S9-69
The ductile-to-brittle transition of direct quenched and tempered martensite begins at 243 K, and the impact energy of the superficial region of the steel plate decreases from 104 J (243 K) to 50 J (213 K). In contrast, the ductile-to-brittle transit
Publikováno v:
Journal of Nuclear Materials. 465:774-783
ER 308L and 309LMo were utilized as the filler metals for the groove and overlay welds of a 304L stainless steel substrate, which was prepared via a gas tungsten arc-welding process in multiple passes. U-bend and weight-loss tests were conducted by t
Autor:
R.K. Shiue, Cheng Yen Wang
Publikováno v:
Advanced Materials Research. 1101:99-103
The purpose of this research is focused on vacuum furnace brazing Incoloy 800 (IN-800) using the copper filler foil. Microstructural evolution and shear strength of brazed joints for various brazing conditions has been evaluated in the experiment. Th
Publikováno v:
Advanced Materials Research. 1101:438-441
The purpose of this investigation is focused on the welding process simulation using the SYSWELD software. It has been used to conduct the simulation of the tungsten inert gas (TIG) welding process. 316L stainless steel (316L SS) is welded with a low